| EFFECT OF LOADING RATE ON NANOINDENTATION CREEP PROPERTIES OF Al FILMS |
| WANG Fei; XU Kewei |
| State Key Laboratory for Mechanical Behavior of Materials; Xi'an Jiaotong University; Xi'an 710049 |
|
Cite this article:
WANG Fei; XU Kewei. EFFECT OF LOADING RATE ON NANOINDENTATION CREEP PROPERTIES OF Al FILMS. Acta Metall Sin, 2004, 40(11): 1138-1142 .
|
|
|
|
|
Received: 17 November 2003
|
|
|
[1] Cui CH Y, Guo J T, Qi Y H, Ye H Q. Acta Metall Sin, 2002; 4: 342(崔传勇,郭建亭,齐义辉,叶恒强.金属学报,2002;4:342) [2] Xiao B L, Ma ZH Y, Bi J. Acta Metall Sin, 2002; 9: 994(肖伯律,马宗义,毕敬.金属学报,2002;9:994) [3] Lucas B N, Oliver W C. Metall Mater Trans A, 1999; 30:601 [4] Chen J, Wang W, Lu L, Lu K. Acta Metall Sin, 2001; 11:1179 (陈 吉,汪 伟,卢 磊,卢 柯.金属学报, 2001;11:1179) [5] Mayo M J, Nix W D. Ada Metall, 1988; 36: 2183 [6] Lafontaine W R, Yost B, Black R D, Li C Y. J Mater Res,1990; 5: 217 [7] Mayo M J, Siegel R W, Liao Y X, Nix W D. J Mater Res,1992; 7: 973 [8] Mayo M J, Siegel R W, Narayanasamy A, Nix W D. JMater Res, 1990; 5: 1073 [9] Raman V, Berriche R. J Mater Res, 1992; 7: 627 [10] Li W B, Henshall J L, Hooper R M, Eastering E. AdaMetall, 1991; 39: 3099 [11] Chang H, Alstetter C J, Averback R. S. J Mater Res, 1992;7: 2962 [12] Li W B, Henshall J L, Hooper R M, Eastering E. AdaMetall, 1991; 39: 3099 [13] Shen B L, Itoi T, Yamasaki T, Ogino Y. Scr Mater, 2000;42: 893 [14] Wu T W, Moshref M, Alexopoulos P S. Thin Solid Films,1990; 187: 295 [15] Langdon T G. Met Forum, 1978; 1: 59 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|