Please wait a minute...
Acta Metall Sin  2026, Vol. 62 Issue (7): 1189-1206    DOI: 10.11900/0412.1961.2025.00418
Overview Current Issue | Archive | Adv Search |
Research Progress and Trends in Characterization Techniques for Ultra-High-Strength and Ultra-Fine Stainless Steel Wires: A Perspective Review
YANG He1,2, HOU Ziyong1,2,3(), HU Xingyi1, CHENG Jinjun1, WANG Yaru1, FAN Guohua4(), HUANG Xiaoxu2,3()
1 International Joint Laboratory for Light Alloys (Ministry of Education), Chongqing University, Chongqing 400044, China
2 State Key Laboratory of Mechanical Transmission for Advanced Equipment, Chongqing University, Chongqing 400044, China
3 Institute of Frontier Interdisciplinary Studies, Chongqing University, Chongqing 400044, China
4 Research Center for Light High-performance Materials, Nanjing Tech University, Nanjing 211816, China
Cite this article: 

YANG He, HOU Ziyong, HU Xingyi, CHENG Jinjun, WANG Yaru, FAN Guohua, HUANG Xiaoxu. Research Progress and Trends in Characterization Techniques for Ultra-High-Strength and Ultra-Fine Stainless Steel Wires: A Perspective Review. Acta Metall Sin, 2026, 62(7): 1189-1206.

Download:  HTML  PDF(3918KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Ultra-high-strength (≥ 3 GPa) and ultra-fine (diameter ≤ 16 μm) stainless steel wires are critical components in solar photovoltaic manufacturing, yet their domestic production poses distinct technical challenges. Countries such as Japan and Germany currently dominate this field, having developed the capability to manufacture wires with tensile strengths of ≥ 3.5 GPa and diameters of ≤ 11 μm. Localizing ultra-high-strength and ultra-fine stainless steel wire technology has therefore become an urgent priority. The extreme true strain and fine diameter attained through cold drawing produce a complex three-dimensional lamellar and heterogeneous microstructure that conventional two-dimensional characterization techniques cannot fully capture. Moreover, the absence of systematic three-dimensional characterization methodologies and standards further impedes localization efforts. This study presents a comprehensive overview of the characterization techniques currently employed for ultra-fine metallic wires and critically evaluates existing approaches for analyzing microstructure, mechanical properties, and performance, along with their respective limitations and strengths. The study also identifies opportunities for developing multiscale, three-dimensional in situ characterization techniques that would provide essential technical support and a theoretical foundation for optimizing wire performance and advancing localization.

Key words:  ultra-fine wire      characterization technique      microstructure      mechanical property      performance      three-dimensional orientation mapping in TEM     
Received:  23 December 2025     
ZTFLH:  TG142.1  
Fund: National Key Research and Development Program of China(2024YFB3713703)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2025.00418     OR     https://www.ams.org.cn/EN/Y2026/V62/I7/1189

MaterialDiameter / μmCharacterization methodRef.
NiTi alloy5-20TEM[24]
316L8-190TEM, XRD[26]
Pearlitic steel20-540TEM[7]
2507 DSS216-6000TEM, SEM, EBSD[9]
316L980-5500TEM, TKD[29]
Pearlitic steel200-1650TEM, APFIM[31]
Cu-Al-Ni alloy23-466DSC[30]
CoCrNi MEA2000-15000TEM[32]
Table 1  Samples and characterization methods for phase tra-nsformation behavior research of metallic wires with different diameters[7,9,24,26,29-32]
Fig.1  Preparation processes of samples for phase transformation research of metallic wires and ultra-fine wires
(a, b) methods for obtaining 3 mm-diameter thin slices for wires with different diameters by nickel plating/copper plating (a) and other methods (b)
(c) twin-jet electropolishing (d) ion milling (e) focused ion beam (FIB)
Fig.2  Summary of inclusion and precipitate characterizations in metallic wires[9,13,24,26,29,32,38,47,48,53-56] (Arrow in Fig.2a represents nano-scale inclusions) (a), and preparation process of 3DAPT needle specimen[38] (b)
Fig.3  Simulations and TEM analyses of dislocations in different materials
(a) three-dimensional (3D) dislocation dynamics simulation results of dislocation microstructures for 600 nm diameter micropillars under tension after torsion[65] (Red arrows and purple arrows indicate single arm operations and interactions between pre-existing dislocations and nucleated dislocations, respectively)
(b) HRTEM images showing the structure of two dislocation cell boundaries in the ferrite lamellae at a strain of 5.4[46] (Frames and arrows show the dislocation core areas and extra atom planes, respectively)
(c) longitudinal TEM images revealing the dislocation arrangements of the sections of a 6.3 μm compressed pillar[76] and a deformed W-coated pillar[75]
(d1, d2) 3D character map showing the distribution of edge components around dislocation loop (d1) and 3D deviation map showing the deviation of local dislocation segments from the respective slip planes (1¯11) and (111¯) (d2)[81] (Inset in Fig.3d1 is TEM image of a top-viewed dislocation loop with b = a / 2[101]. b —Burgers vector, a—lattice constant)
Fig.4  Characterizations of grain size in metallic wires and ultra-fine wires[9,21,92] (a-e) and schematic of sampling positions in wire sample preparation (f)
(a-c) OM (a)[92], SEM (b), and EBSD (c)[21] images showing grain size of wires
(d, e) TEM images of ferrite and austenite in 2507 DSS wires at ε = 5.01 (d) and ε = 6.65 (e)[9] (ε—strain)
Fig.5  Characterizations and schematic of grain boundaries in metallic wires and ultra-fine wires (a, a1, a2) nanobeam diffraction patterns (a), TEM image (a1), and schematic (a2) of numbered cells in the ferrite lamellae at a strain of 5.4[46] (Solid lines and dashed lines in Figs.5a1 and a2 represent cementite lamellae and dislocation cell boundaries, respectively) (b) TEM images and SAED pattern (inset) of the CoCrNi wire showing that the nano-twins could be cut up by the other direction micro-band after tensile test at liquid-nitrogen temperature[32] (c) phase maps showing subgrain boundaries obtained via scanning nano-beam TEM diffraction for heat-treated nanocrystalline hypereutectoid steel wires in the transverse cross-section[72] (d) overlay of projected 3D atom map and bright-field STEM image of a pearlitic steel atom probe specimen[17] (Insets are corresponding nanobeam diffraction patterns. GB2—Σ3 coherent twin)
Fig.6  Analyses of textures in metallic wires and ultra-fine wires
(a) schematical positions showing orientation of 111 crystallographic axis of the grains with respect to the wire axis for a fractured wire[102]
(b) schematical positions of EBSD maps and corresponding inverse pole figures near the edge and central region of the wires[102]
(c) schematics of SEM sampling positions of a drawn fine high carbon steel wire[45] (ND—normal direction, TD—transverse direction, RD—rolling direction, W—width)
(d) summary of texture study in wires and ultra-fine wires[14,15,20,29,45,69,71,90,96,111-116] (NBD—nanobeam electron diffraction, SXRD—synchrotron X-ray diffraction, VPSC—visco-plastic self-consistent)
TypeMethodMaterialDiameter μmResolutionSize effectRef.
Tension test-304 SS/316 SS≥ 108.33 × 10-4 s-1-Our work
-2205 DSS≥ 10001 × 10-3 s-1Strong[21]
-Iron68-12003.33 × 10-4 s-1Strong[96]
-316L SS61-2001 × 10-3 s-1Strong[18]
-Steel≥ 8.851 × 10-3 s-1Strong[98]
Hardness test-HEA≥ 740Load: 1 kgf-[56]
-HEA≥ 1000Load: 0.05-0.5 kgf-[117]
-Metal~50--[118]
Torsion testFiber-based torsion balanceCu12-170∼1.5 μN·cmStrong[61]
Cu16-1800.13-2.35 μN·cmNone[119]
Modified fiber-based torsion balanceCu18-1050.03-0.17 μN·cmStrong[63]
-Metal≤ 10000--[120]
-316 SS≥ 200~0.12 μN·cm-[121]
Table 2  Methods and results of mechanical properties of metallic wires and ultra-fine wires[18,21,56,61,63,96,98,117-121]
Fig.7  Three-dimensional orientation mapping in TEM (3D-OMiTEM) characterizations of texture in ultra-fine wires
(a) reconstructed 3D orientation map of the gold nanoparticle film[166] (mrd—multiples of random distribution)
(b) 3D-OMiTEM characterization of the deformation-induced structure changes in nanograined nickel[168]
[1] Chen J W, Fu S F, Ni R L, et al. Electron-beam interference and Fresnel diffraction [J]. Acta Opt. Sin., 1986, 6: 23
陈建文, 傅淑芬, 倪瑞莲 等. 电子束干涉和菲涅耳衍射 [J]. 光学学报, 1986, 6: 23
[2] Toshizo T. Rebar and wire at the forefront of high strength [J]. Nippon Steel Mon., 2006, 26: 9
樽井 敏三. 高強度の最先端をいく棒鋼 線材[J]. モノづくりの原点-科学の世界, 2006, 26: 9
[3] Embury J D, Fisher R M. The structure and properties of drawn pearlite [J]. Acta Metall., 1966, 14: 147
doi: 10.1016/0001-6160(66)90296-3
[4] Chen X X, Ngan A H W. Specimen size and grain size effects on tensile strength of Ag microwires [J]. Scr. Mater., 2011, 64: 717
doi: 10.1016/j.scriptamat.2010.12.031
[5] Gao X Q, Hu W C, Gao Y S. Preparation of ultrafine tungsten wire via electrochemical method in an ionic liquid [J]. Fusion Eng. Des., 2013, 88: 23
doi: 10.1016/j.fusengdes.2012.09.022
[6] Gan Z P, He Y M, Liu D B, et al. Hall-Petch effect and strain gradient effect in the torsion of thin gold wires [J]. Scr. Mater., 2014, 87: 41
doi: 10.1016/j.scriptamat.2014.05.011
[7] Li Y J, Raabe D, Herbig M, et al. Segregation stabilizes nanocrystalline bulk steel with near theoretical strength [J]. Phys. Rev. Lett., 2014, 113: 106104
doi: 10.1103/PhysRevLett.113.106104
[8] Zhang X D. Quantitative investigation of microstructural evolution during cold wire drawing of a pearlitic steel wire and its relationship with mechanical properties [D]. Beijing: Tsinghua University, 2009
张晓丹. 钢帘线钢丝冷拉拔过程中组织演变的定量研究与力学性能 [D]. 北京: 清华大学, 2009
[9] Li Q, Zhou L C, Gao H, et al. Ultra-strong cold-drawn 2507 stainless steel wire with heterogenous microstructure of dual-phase and grain size [J]. J. Mater. Res. Technol., 2024, 33: 6876
doi: 10.1016/j.jmrt.2024.11.087
[10] Tarui T, Maruyama N, Takahashi J, et al. Microstructure control and strengthening of high-carbon steel wires [J]. Nippon Steel Tech. Rep., 2005, 56
[11] Dunstan D J, Bushby A J. Theory of deformation in small volumes of material [J]. Proc. Roy. Soc., 2004, 460A: 2781
[12] Raabe D, Choi P P, Li Y J, et al. Metallic composites processed via extreme deformation: Toward the limits of strength in bulk materials [J]. MRS Bull., 2010, 35: 982
doi: 10.1557/mrs2010.703
[13] Languillaume J, Kapelski G, Baudelet B. Cementite dissolution in heavily cold drawn pearlitic steel wires [J]. Acta Mater., 1997, 45: 1201
doi: 10.1016/S1359-6454(96)00216-9
[14] Feng H C, Wang L F, Cui S Y, et al. Microstructure and strengthening mechanisms of nanolamellar structures in ultrastrong drawn iron wires [J]. Scr. Mater., 2021, 200: 113906
doi: 10.1016/j.scriptamat.2021.113906
[15] Arya A, Suwas S, Chokshi A H. Strengthening in tension and weakening in torsion in drawn nickel microwires [J]. Mater. Sci. Eng., 2022, A856: 143955
[16] Li Y J, Choi P, Borchers C, et al. Atom probe tomography characterization of heavily cold drawn pearlitic steel wire [J]. Ultramicroscopy, 2011, 111: 628
doi: 10.1016/j.ultramic.2010.11.010 pmid: 21146309
[17] Herbig M, Raabe D, Li Y J, et al. Atomic-scale quantification of grain boundary segregation in nanocrystalline material [J]. Phys. Rev. Lett., 2014, 112: 126103
doi: 10.1103/PhysRevLett.112.126103
[18] Fu S C, Yu D J, Chen Y, et al. Size effect in stainless steel thin wires under tension [J]. Mater. Sci. Eng., 2020, A790: 139686
[19] Guo S, He Y M, Lei J, et al. Individual strain gradient effect on torsional strength of electropolished microscale copper wires [J]. Scr. Mater., 2017, 130: 124
doi: 10.1016/j.scriptamat.2016.11.029
[20] Fang F, Wang L P, Zhou L C, et al. Application of texture inheritance on manufacturing ultra-high strength pearlitic steel wire [J]. Mater. Sci. Technol., 2018, 34: 766
doi: 10.1080/02670836.2017.1393999
[21] Wang Y, Zhou L C, Shi C J, et al. Synergistic twinning and deformation-induced martensite transition facilitating 3GPa duplex stainless steel wire prepared by drawing [J]. Mater. Sci. Eng., 2024, A916: 147379
[22] Liu D B, He Y M, Dunstan D J, et al. Toward a further understanding of size effects in the torsion of thin metal wires: An experimental and theoretical assessment [J]. Int. J. Plast., 2013, 41: 30
doi: 10.1016/j.ijplas.2012.08.007
[23] Lan L Y, Kong X W, Qiu C L, et al. A review of recent advance on hydrogen embrittlement phenomenon based on multiscale mechanical experiments [J]. Acta Metall. Sin., 2021, 57: 845
doi: 10.11900/0412.1961.2020.00378
兰亮云, 孔祥伟, 邱春林 等. 基于多尺度力学实验的氢脆现象的最新研究进展 [J]. 金属学报, 2021, 57: 845
doi: 10.11900/0412.1961.2020.00378
[24] Norfleet D M, Sarosi P M, Manchiraju S, et al. Transformation-induced plasticity during pseudoelastic deformation in Ni-Ti microcrystals [J]. Acta Mater., 2009, 57: 3549
doi: 10.1016/j.actamat.2009.04.009
[25] Gavriljuk V G. Decomposition of cementite in pearlitic steel due to plastic deformation [J]. Mater. Sci. Eng., 2003, A345: 81
[26] Wang H S, Yang J R, Bhadeshia H K D H. Characterisation of severely deformed austenitic stainless steel wire [J]. Mater. Sci. Technol., 2005, 21: 1323
doi: 10.1179/174328405X63980
[27] Ye J, Mishra R K, Pelton A R, et al. Direct observation of the NiTi martensitic phase transformation in nanoscale volumes [J]. Acta Mater., 2010, 58: 490
doi: 10.1016/j.actamat.2009.09.027
[28] Xu L X, Zhou L H, Bi H Y, et al. Modeling of strain-induced γ → α′ phase transformation for 201Cu metastable austenitic stainless steel and its verification in rolling processes [J]. J. Iron Steel Res. Int., 2024, 31: 2248
doi: 10.1007/s42243-023-01152-8
[29] Li Q, Zhou L C, Pan Y J, et al. Formation of nano martensite grain with specific angle grain boundary during the drawing process of 316L stainless steel [J]. Mater. Sci. Eng., 2024, A897: 146309
[30] Chen Y, Schuh C A. Size effects in shape memory alloy microwires [J]. Acta Mater., 2011, 59: 537
doi: 10.1016/j.actamat.2010.09.057
[31] Hong M H, Reynolds W T, Tarui T, et al. Atom probe and transmission electron microscopy investigations of heavily drawn pearlitic steel wire [J]. Metall. Mater. Trans., 1999, 30A: 717
[32] Liu J P, Chen J X, Liu T W, et al. Superior strength-ductility CoCrNi medium-entropy alloy wire [J]. Scr. Mater., 2020, 181: 19
doi: 10.1016/j.scriptamat.2020.02.002
[33] Wang J Z, Tang H P, Qian M, et al. Fabrication of high strength and ductile stainless steel fiber felts by sintering [J]. JOM, 2016, 68: 890
doi: 10.1007/s11837-015-1803-z
[34] Borchers C, Lehmberg A, Deutges M, et al. Effect of annealing on point defect population in cold-drawn pearlitic steel wires [J]. Scr. Mater., 2014, 86: 17
doi: 10.1016/j.scriptamat.2014.04.016
[35] Choi J Y, Jin W. Strain induced martensite formation and its effect on strain hardening behavior in the cold drawn 304 austenitic stainless steels [J]. Scr. Mater., 1997, 36: 99
doi: 10.1016/S1359-6462(96)00338-7
[36] Zhao X Y, Liu Y, Wang Y, et al. Recrystallization and grain growth of 316L stainless steel wires [J]. Metall. Mater. Trans. A, 2014, 45A: 3446
[37] Zhou T, Babu R P, Hou Z Y, et al. On the role of transmission electron microscopy for precipitation analysis in metallic materials [J]. Crit. Rev. Solid State Mater. Sci., 2022, 47: 388
doi: 10.1080/10408436.2021.1941751
[38] Takahashi J, Tarui T, Kawakami K. Three-dimensional atom probe analysis of heavily drawn steel wires by probing perpendicular to the pearlitic lamellae [J]. Ultramicroscopy, 2009, 109: 193
doi: 10.1016/j.ultramic.2008.10.013 pmid: 19070959
[39] Barna A, Pécz B, Menyhard M. Amorphisation and surface morphology development at low-energy ion milling [J]. Ultramicroscopy, 1998, 70: 161
doi: 10.1016/S0304-3991(97)00120-4
[40] Raffa V, Castrataro P, Menciassi A, et al. Focused ion beam as a scanning probe: methods and applications [A]. Applied Scanning Probe Methods II [M]. Berlin, Heidelberg: Springer 2006: 361
[41] Raabe D, Mattissen D. Microstructure and mechanical properties of a cast and wire-drawn ternary Cu-Ag-Nb in situ composite [J]. Acta Mater., 1998, 46: 5973
doi: 10.1016/S1359-6454(98)00218-3
[42] Raabe D, Mattissen D. Experimental investigation and Ginzburg-Landau modeling of the microstructure dependence of superconductivity in Cu-Ag-Nb wires [J]. Acta Mater., 1999, 47: 769
doi: 10.1016/S1359-6454(98)00406-6
[43] Pelton A R, Laabs F C, Spitzig W A, et al. Microstructural analysis of in-situ Cu-Nb composite wires [J]. Ultramicroscopy, 1987, 22: 251
doi: 10.1016/0304-3991(87)90069-6
[44] Jafari M, Bang C W, Han J C, et al. Evolution of microstructure and tensile properties of cold-drawn hyper-eutectoid steel wires during post-deformation annealing [J]. J. Mater. Sci. Technol., 2020, 41: 1
doi: 10.1016/j.jmst.2019.08.054
[45] Gondo S, Tanemura R, Suzuki S, et al. Microstructures and mechanical properties of fiber textures forming mesoscale structure of drawn fine high carbon steel wire [J]. Mater. Sci. Eng., 2019, A747: 255
[46] Zhang X D, Hansen N, Godfrey A, et al. Dislocation-based plasticity and strengthening mechanisms in sub-20 nm lamellar structures in pearlitic steel wire [J]. Acta Mater., 2016, 114: 176
doi: 10.1016/j.actamat.2016.04.040
[47] Danoix F, Julien D, Sauvage X, et al. Direct evidence of cementite dissolution in drawn pearlitic steels observed by tomographic atom probe [J]. Mater. Sci. Eng., 1998, A250: 8
[48] Zelin M. Microstructure evolution in pearlitic steels during wire drawing [J]. Acta Mater., 2002, 50: 4431
doi: 10.1016/S1359-6454(02)00281-1
[49] Wang Y D, Li R G, Nie Z H, et al. A review on the application of neutron and high-energy X-ray diffraction characterization methods in engineering materials [J]. Chin. J. Eng., 2022, 44: 676
王沿东, 李润光, 聂志华 等. 中子/同步辐射衍射表征技术及其在工程材料研究中的应用 [J]. 工程科学学报, 2022, 44: 676
[50] Liu Y Z, Meng B, Wan M. Deformation characteristics and performance evolution of superalloy capillary drawn by electrically assisted microforming [J]. Int. J. Mech. Sci., 2023, 240: 107912
doi: 10.1016/j.ijmecsci.2022.107912
[51] Hu X J, Shen K, Ju Y F, et al. Research and development of high carbon steel wire rod for 36 μm, 5000 MPa grade ultra-fine steel wire [J]. China Metall., 2025, 35(11): 145
胡显军, 沈 奎, 居寅飞 等. 36 μm 5000 MPa级超细钢丝用高碳钢盘条的研发 [J]. 中国冶金, 2025, 35(11): 145
[52] TesaŘ K, BalÍK K, Sucharda Z, et al. Direct extrusion of thin Mg wires for biomedical applications [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 373
doi: 10.1016/S1003-6326(20)65219-0
[53] Hong S I. Yield strength of a heavily drawn Cu-20% Nb filamentary microcomposite [J]. Scr. Mater., 1998, 39: 1685
doi: 10.1016/S1359-6462(98)00383-2
[54] Shyr T W, Shie J W, Huang S J, et al. Phase transformation of 316L stainless steel from wire to fiber [J]. Mater. Chem. Phys., 2010, 122: 273
doi: 10.1016/j.matchemphys.2010.02.048
[55] Yang S T, Hwang W S, Shyr T W, et al. Evolution of magnetic phase at low aging temperature in a heavily cold-drawn stainless steel fiber [J]. J. Magn. Magn. Mater., 2012, 324: 2388
doi: 10.1016/j.jmmm.2012.03.007
[56] Shim S H, Pouraliakbar H, Hong S I. High strength dual fcc phase CoCuFeMnNi high-entropy alloy wires with dislocation wall boundaries stabilized by phase boundaries [J]. Mater. Sci. Eng., 2021, A825: 141875
[57] Li Y J, Choi P, Borchers C, et al. Atomic-scale mechanisms of deformation-induced cementite decomposition in pearlite [J]. Acta Mater., 2011, 59: 3965
doi: 10.1016/j.actamat.2011.03.022
[58] Maruyama N, Tarui T, Tashiro H. Atom probe study on the ductility of drawn pearlitic steels [J]. Scr. Mater., 2002, 46: 599
doi: 10.1016/S1359-6462(02)00037-4
[59] Xu Z K, Wang P, Zhang P, et al. Fatigue strength optimization of high-strength steels by precisely controlling microstructure and inclusions [J]. J. Mater. Sci. Technol., 2025, 230: 165
doi: 10.1016/j.jmst.2025.01.018
[60] Raabe D, Ohsaki S, Hono K. Mechanical alloying and amorphization in Cu-Nb-Ag in situ composite wires studied by transmission electron microscopy and atom probe tomography [J]. Acta Mater., 2009, 57: 5254
doi: 10.1016/j.actamat.2009.07.028
[61] Fleck N A, Muller G M, Ashby M F, et al. Strain gradient plasticity: Theory and experiment [J]. Acta Metall. Mater., 1994, 42: 475
doi: 10.1016/0956-7151(94)90502-9
[62] Abu Al-Rub R K, Voyiadjis G Z. A physically based gradient plasticity theory [J]. Int. J. Plast., 2006, 22: 654
doi: 10.1016/j.ijplas.2005.04.010
[63] Liu D B, He Y M, Tang X T, et al. Size effects in the torsion of microscale copper wires: Experiment and analysis [J]. Scr. Mater., 2012, 66: 406
doi: 10.1016/j.scriptamat.2011.12.003
[64] Zbib H M, Aifantis E C. Size effects and length scales in gradient plasticity and dislocation dynamics [J]. Scr. Mater., 2003, 48: 155
doi: 10.1016/S1359-6462(02)00342-1
[65] Gravell J D, Ryu I. Latent hardening/softening behavior in tension and torsion combined loadings of single crystal FCC micropillars [J]. Acta Mater., 2020, 190: 58
doi: 10.1016/j.actamat.2020.02.030
[66] Bai Z W, Ding Z G, Zhou A L, et al. Molecular dynamics simulation of thermo-kinetics of tensile deformation of α-Fe single crystal [J]. Acta Metall. Sin., 2024, 60: 848
柏智文, 丁志刚, 周爱龙 等. α-Fe单晶拉伸变形热-动力学的分子动力学模拟 [J]. 金属学报, 2024, 60: 848
doi: 10.11900/0412.1961.2022.00606
[67] Guo X X, Shuai M R, Chu Z B, et al. Microstructure evolution near interface and the element diffusion dynamics of the composite stainless steel rebar [J]. Acta Metall. Sin., 2025, 61: 336
doi: 10.11900/0412.1961.2023.00032
郭星星, 帅美荣, 楚志兵 等. 不锈钢复合钢筋近界面微观组织演变及元素扩散动力学 [J]. 金属学报, 2025, 61: 336
doi: 10.11900/0412.1961.2023.00032
[68] Wang D, Xu L Y, Zhao L, et al. Phase field and crystal plasticity simulation of irradiation-induced he bubbles evolution and mechanical behavior in 316H steel and weld metal [J]. Acta Metall. Sin., 2026, 62: 173
doi: 10.11900/0412.1961.2025.00239
王 栋, 徐连勇, 赵 雷 等. 316H钢及其焊缝金属辐照He泡演化与力学行为的相场-晶体塑性耦合模拟 [J]. 金属学报, 2026, 62: 173
[69] Arya A, Suwas S, Gérard C, et al. Strength and microstructure evolution in nickel during large strain wire drawing [J]. Acta Mater., 2021, 221: 117396
doi: 10.1016/j.actamat.2021.117396
[70] Zhu Y L, Cao Y, Xu B Y, et al. Deep learning-enhanced cellular automaton framework for modeling static recrystallization behavior [J]. J. Mater. Inf., 2025, 5: 55
[71] Liu J S, Zhou Y, Wang S W, et al. Exploring the evolution of texture and properties of ultrafine copper wire during high strain drawing process [J]. J. Cent. South Univ., 2025, 32: 1973
doi: 10.1007/s11771-025-5896-4
[72] Li Y J, Kostka A, Choi P, et al. Mechanisms of subgrain coarsening and its effect on the mechanical properties of carbon-supersaturated nanocrystalline hypereutectoid steel [J]. Acta Mater., 2015, 84: 110
doi: 10.1016/j.actamat.2014.10.027
[73] Read H G, Reynolds W T, Hono K, et al. APFIM and TEM studies of drawn pearlitic wire [J]. Scr. Mater., 1997, 37: 1221
doi: 10.1016/S1359-6462(97)00223-6
[74] Uchic M D, Dimiduk D M, Florando J N, et al. Sample dimensions influence strength and crystal plasticity [J]. Science, 2004, 305: 986
pmid: 15310897
[75] Ng K S, Ngan A H W. Effects of trapping dislocations within small crystals on their deformation behavior [J]. Acta Mater., 2009, 57: 4902
doi: 10.1016/j.actamat.2009.06.053
[76] Ng K S, Ngan A H W. Stochastic nature of plasticity of aluminum micro-pillars [J]. Acta Mater., 2008, 56: 1712
doi: 10.1016/j.actamat.2007.12.016
[77] Rao S I, Dimiduk D M, Tang M, et al. Estimating the strength of single-ended dislocation sources in micron-sized single crystals [J]. Philos. Mag., 2007, 87: 4777
doi: 10.1080/14786430701591513
[78] Kiener D, Motz C, Rester M, et al. FIB damage of Cu and possible consequences for miniaturized mechanical tests [J]. Mater. Sci. Eng., 2007, A459: 262
[79] Kiener D, Grosinger W, Dehm G, et al. A further step towards an understanding of size-dependent crystal plasticity: In situ tension experiments of miniaturized single-crystal copper samples [J]. Acta Mater., 2008, 56: 580
doi: 10.1016/j.actamat.2007.10.015
[80] Shan Z W, Mishra R K, Syed Asif S A, et al. Mechanical annealing and source-limited deformation in submicrometre-diameter Ni crystals [J]. Nat. Mater., 2008, 7: 115
pmid: 18157134
[81] Fu R, Feng Z Q, Huang X X. Orientation distribution and deviation behaviors of dislocation loops in a quenched Al-Cu alloy [J]. Acta Mater., 2024, 270: 119837
doi: 10.1016/j.actamat.2024.119837
[82] Wang T M, Wang K, Zhu J, et al. Applications of synchrotron microradiography in materials science——In situ visualization of the growth of metallic alloy crystals [J]. Physics, 2012, 41: 244
王同敏, 王 琨, 朱 晶 等. 同步辐射成像技术在材料科学中的应用——金属合金晶体生长原位可视化 [J]. 物理, 2012, 41: 244
[83] Huang L L, Qin J, Huang J L, et al. Effect of Zr on microstructure and mechanical properties of 304 stainless steel joints brazed by Ag-Cu-Sn-In filler metal [J]. J. Iron Steel Res. Int., 2024, 31: 2448
doi: 10.1007/s42243-024-01339-7
[84] Yang B, Motz C, Grosinger W, et al. Tensile behaviour of micro-sized copper wires studied using a novel fibre tensile module [J]. Int. J. Mater. Res., 2008, 99: 716
doi: 10.3139/146.101690
[85] Xu Q H, Zhu J X, Zong Y, et al. Effect of drawing and annealing on the microstructure and mechanical properties of 304 austenitic stainless steel wire [J]. Mater. Res. Express, 2021, 8: 126530
doi: 10.1088/2053-1591/ac44d6
[86] Dai T, Gu D Y, Qiu Y W, et al. An experimental study on effects of temperature gradient on microstructure of a 308L stainless steel manufactured by directed energy deposition [J]. J. Iron Steel Res. Int., 2024, 31: 2031
doi: 10.1007/s42243-023-01158-2
[87] Mojtaba P, Mohammad S, Christof S. Ultra-fine wire fabricating apparatus and method [P]. U.S. Patent, 20170252788, 2017
[88] Fukumaru T, Hidaka H, Tsuchiyama T, et al. Effect of wire diameter and grain size on tensile properties of austenitic stainless steel wire [J]. Tetsu-to-Hagané, 2005, 91: 828
doi: 10.2355/tetsutohagane1955.91.11_828
[89] Liu S F, Xu P, Wang B J. Drawing and property of 316L extra fine stainless steel wires [J]. Mater. Sci. Forum, 2012, 724: 331
doi: 10.4028/www.scientific.net/MSF.724
[90] Yue S P, Li G L, Qu J P, et al. Investigation on the dual-phase co-deformation behavior and strengthening mechanism in cold-drawn Cu-20Fe alloy [J]. Mater. Sci. Eng., 2023, A862: 144474
[91] Liu D B, He Y M, Dunstan D J, et al. Anomalous plasticity in the cyclic torsion of micron scale metallic wires [J]. Phys. Rev. Lett., 2013, 110: 244301
doi: 10.1103/PhysRevLett.110.244301
[92] Yu H O, Wang Y, Liu Y, et al. Grain growth behavior of an as-drawn 316L stainless steel fiber after annealing treatment [J]. Mater. Charact., 2015, 109: 79
doi: 10.1016/j.matchar.2015.09.014
[93] Liu D B, He Y M, Hu P, et al. Characterizing torsional properties of microwires using an automated torsion balance [J]. Exp. Mech., 2017, 57: 297
doi: 10.1007/s11340-016-0212-8
[94] Seitz J M, Utermöhlen D, Wulf E, et al. The manufacture of resorbable suture material from magnesium-drawing and stranding of thin wires [J]. Adv. Eng. Mater., 2011, 13: 1087
doi: 10.1002/adem.v13.12
[95] Chen Y, Kraft O, Walter M. Size effects in thin coarse-grained gold microwires under tensile and torsional loading [J]. Acta Mater., 2015, 87: 78
doi: 10.1016/j.actamat.2014.12.034
[96] Feng H C, Fang F, Zhou X F, et al. Heavily cold drawn iron wires: Role of nano-lamellae in enhancing the tensile strength [J]. Mater. Sci. Eng., 2020, A796: 140017
[97] Guo N, Luan B F, Wang B S, et al. Microstructure and texture evolution in fully pearlitic steel during wire drawing [J]. Sci. China Technol. Sci., 2013, 56: 1139
doi: 10.1007/s11431-013-5184-7
[98] Li Y J, Choi P, Goto S, et al. Evolution of strength and microstructure during annealing of heavily cold-drawn 6.3GPa hypereutectoid pearlitic steel wire [J]. Acta Mater., 2012, 60: 4005
doi: 10.1016/j.actamat.2012.03.006
[99] Zhao Y F, Niverty S, Ma X, et al. 3D grain structure of an extruded 6061 Al alloy by lab-scale X-ray diffraction contrast tomography (DCT) [J]. Mater. Charact., 2020, 170: 110716
doi: 10.1016/j.matchar.2020.110716
[100] Ke Y B, Li B, Duan H P. Morphology and chemical composition of nanoprecipitate in AerMet100 steel by separation of the nuclear and magnetic small-angle neutron scattering data [J]. Acta Metall. Sin., 2024, 60: 1109
doi: 10.11900/0412.1961.2024.00062
柯于斌, 李 彬, 段辉平. 利用小角中子核磁散射分离研究AerMet100钢中纳米析出相的形貌和成分 [J]. 金属学报, 2024, 60: 1109
doi: 10.11900/0412.1961.2024.00062
[101] Troitskiy O A, Stashenko V I. Electroplastic wire drawing: A promising method of production of lightweight wire and cable [J]. J. Mach. Manuf. Reliab., 2015, 44: 758
doi: 10.3103/S1052618815080087
[102] Agepati S, Ghosh P, Chokshi A H. Microstructural evolution and strength variability in microwires [J]. Mater. Sci. Eng., 2016, A652: 239
[103] Liu D B, He Y M, Shen L, et al. Accounting for the recoverable plasticity and size effect in the cyclic torsion of thin metallic wires using strain gradient plasticity [J]. Mater. Sci. Eng., 2015, A647: 84
[104] Kwon Y J, Won J W, Park S H, et al. Ultrahigh-strength CoCrFe-MnNi high-entropy alloy wire rod with excellent resistance to hydrogen embrittlement [J]. Mater. Sci. Eng., 2018, A732: 105
[105] Shen W L, Liao Y X, Wu X Z, et al. Phase-field simulation of grain boundary groove formation [J]. Acta Metall. Sin., 2026, 62: 523
doi: 10.11900/0412.1961.2024.00138
申文龙, 廖宇轩, 吴学志 等. 晶界沟槽形成过程的相场模拟 [J]. 金属学报, 2026, 62: 523
doi: 10.11900/0412.1961.2024.00138
[106] Huang X T, Wang J J, Zhao S X, et al. High-resolution multiscale modeling of mechanical behavior of cold-drawn pearlitic steels [J]. J. Mater. Res. Technol., 2021, 15: 5920
doi: 10.1016/j.jmrt.2021.10.087
[107] Zhang Z Q, Liao X, Ren Z K, et al. Effect of two-pass rolling of textured roll and polished roll on surface topography and mechanical properties of 316L stainless steel ultra-thin strip [J]. J. Iron Steel Res. Int., 2025, 32: 186
doi: 10.1007/s42243-024-01219-0
[108] De Carvalho Paes Loureiro R, Beres M, Masoumi M, et al. The effect of pearlite morphology and crystallographic texture on environmentally assisted cracking failure [J]. Eng. Fail. Anal., 2021, 126: 105450
doi: 10.1016/j.engfailanal.2021.105450
[109] Zhao J W, Xie Q Z, Ma L N, et al. Effect of rolling schedules on ridging resistance of ultra-thin ferritic stainless steel foil [J]. J. Iron Steel Res. Int., 2025, 32: 198
doi: 10.1007/s42243-024-01258-7
[110] Saglik K, Tan X Y, Suwardi A, et al. Texture engineering to boost the thermoelectric properties [J]. Trans. Tianjin Univ., 2023, 29: 189
doi: 10.1007/s12209-023-00354-1
[111] Zhang B, Song Y, Voyiadjis G Z, et al. Assessing texture development and mechanical response in microscale reverse extrusion of copper [J]. J. Mater. Res., 2018, 33: 978
doi: 10.1557/jmr.2018.22
[112] Guo S, He Y M, Liu D B, et al. Geometrically necessary dislocations induced size effect in the torsional stress relaxation behavior of thin metallic wires [J]. Scr. Mater., 2019, 173: 129
doi: 10.1016/j.scriptamat.2019.08.002
[113] Troitsky O A, Stashenko V I. Advantages of drawing and rolling metals with pulse current [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2020, 848: 012084
[114] Nienaber M, Yi S, Kainer K U, et al. On the direct extrusion of magnesium wires from Mg-Al-Zn series alloys [J]. Metals, 2020, 10: 1208
doi: 10.3390/met10091208
[115] Bai J, Xu Y, Fan Q Z, et al. Mechanical properties and degradation behaviors of Zn-xMg alloy fine wires for biomedical applications [J]. Scanning, 2021, 2021: 4831387
[116] Feng H C, Cai L, Wang L F, et al. Microstructure and strength in ultrastrong cold-drawn medium carbon steel [J]. J. Mater. Sci. Technol., 2022, 97: 89
doi: 10.1016/j.jmst.2021.04.027
[117] Cho H S, Bae S J, Na Y S, et al. Influence of reduction ratio on the microstructural evolution and subsequent mechanical properties of cold-drawn Co10Cr15Fe25Mn10Ni30V10 high entropy alloy wires [J]. J. Alloys Compd., 2020, 821: 153526
doi: 10.1016/j.jallcom.2019.153526
[118] Yeung J, Keong L C. Hardness measurement of copper bonding wire [J]. Procedia Eng., 2014, 75: 134
doi: 10.1016/j.proeng.2013.11.029
[119] Lu W Y, Song B. Quasi-static torsion characterization of micro-diameter copper wires [J]. Exp. Mech., 2011, 51: 729
doi: 10.1007/s11340-010-9377-8
[120] Aviation Industry Corporation of China. Metal wire torsion test method [S]. Beijing: Aviation Industry Press, 1996
中国航空工业总公司. 金属丝材扭转试验方法 [S]. 北京: 航空工业出版社, 1996
[121] Shen Y, Fu S, Shi S, et al. Torsional fatigue with axial constant stress of oligo-crystalline 316L stainless steel thin wire [J]. Fatigue Fract. Eng. Mater. Struct., 2018, 41: 1929
doi: 10.1111/ffe.v41.9
[122] Xie Y Y, Lei J, Hua F F, et al. Size and passivation effects in the torsion of thin metallic wires [J]. Acta Mech. Sin., 2023, 39: 422346
doi: 10.1007/s10409-022-22346-x
[123] Cunha F G, Santos T G, Xavier J. In situ monitoring of wire and arc additive manufacturing by digital image correlation: A case study [J]. Procedia Struct. Integrity, 2022, 37: 33
[124] Chinh N Q, Csanádi T, Győri T, et al. Strain rate sensitivity studies in an ultrafine-grained Al-30wt.% Zn alloy using micro- and nanoindentation [J]. Mater. Sci. Eng., 2012, A543: 117
[125] Oliver W C, Pharr G M. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments [J]. J. Mater. Res., 1992, 7: 1564
doi: 10.1557/JMR.1992.1564
[126] Kiener D, Rester M, Scheriau S, et al. Influence of external and internal length scale on the flow stress of copper [J]. Int. J. Mater. Res., 2007, 98: 1047
doi: 10.3139/146.101578
[127] Song L Y, Wang C C, Li Y Z, et al. Predicting stacking fault energy in austenitic stainless steels via physical metallurgy-based machine learning approaches [J]. J. Mater. Inf., 2025, 5: 2
[128] Chen B, Xun Y, Wang S F, et al. Horizontal-type test apparatus and test method for measuring torsion property of material under electron microscope [P]. China Patent, 107219133A, 2019
陈 博, 郇 勇, 王素芳 等. 一种在电镜下测量材料扭转性能的横式测试装置及测试方法 [P]. 中国专利, 107219133A, 2019)
[129] Sumigawa T, Byungwoon K, Mizuno Y, et al. In situ observation on formation process of nanoscale cracking during tension-compression fatigue of single crystal copper micron-scale specimen [J]. Acta Mater., 2018, 153: 270
doi: 10.1016/j.actamat.2018.04.061
[130] Yan Y, Chen W, Sumigawa T, et al. A quantitative in situ SEM bending method for stress relaxation of microscale materials at room temperature [J]. Exp. Mech., 2020, 60: 937
doi: 10.1007/s11340-020-00611-7
[131] Li R, Zuo X W, Wang E G. Influence of thermomechanical process and Fe addition on microstructural evolution and properties of Cu-26 wt%Ag composite [J]. J. Alloys Compd., 2019, 773: 121
doi: 10.1016/j.jallcom.2018.09.179
[132] Martinez-Perez M L, Mompean F J, Ruiz-Hervias J, et al. Residual stress profiling in the ferrite and cementite phases of cold-drawn steel rods by synchrotron X-ray and neutron diffraction [J]. Acta Mater., 2004, 52: 5303
doi: 10.1016/j.actamat.2004.07.036
[133] Toribio J, Kharin V, Lorenzo M, et al. Role of drawing-induced residual stresses and strains in the hydrogen embrittlement susceptibility of prestressing steels [J]. Corros. Sci., 2011, 53: 3346
doi: 10.1016/j.corsci.2011.06.012
[134] Zand R Z, Verbeken K, Adriaens A. Electrochemical assessment of the self-healing properties of cerium doped sol-gel coatings on 304L stainless steel substrates [J]. Int. J. Electrochem. Sci., 2012, 7: 9592
doi: 10.1016/S1452-3981(23)16222-5
[135] Ding L, Zhang H B, Wang R J, et al. Enhanced corrosion resistance and electrical conductivity of stainless steel bipolar plates by molybdenum ion implantation [J]. J. Iron Steel Res. Int., 2025, 32: 1073
doi: 10.1007/s42243-024-01296-1
[136] Xie H, Lei Y N, Tang G J, et al. Microstructure and oxidation behavior of composite Co-W/NiO coating on ferritic stainless steel for SOFC interconnector [J]. J. Iron Steel Res. Int., 2025, 32: 1139
[137] Dou G X, Guo H J, Guo J, et al. Effect of slag composition on kinetic behavior of deep deoxidation of 5 wt.% Si high-silicon austenitic stainless steel [J]. J. Iron Steel Res. Int., 2024, 31: 1873
doi: 10.1007/s42243-024-01250-1
[138] Zheng J H, Feng Y, Zhao Y, et al. High-temperature oxidation behavior and mechanism of 18Cr-Mo-type ferritic stainless steel containing W and Ce in simulated automotive exhaust gas [J]. J. Iron Steel Res. Int., 2025, 32: 2116
doi: 10.1007/s42243-024-01368-2
[139] Bai J, Yin L L, Lu Y, et al. Preparation, microstructure and degradation performance of biomedical magnesium alloy fine wires [J]. Prog. Nat. Sci.: Mater. Int., 2014, 24: 523
doi: 10.1016/j.pnsc.2014.08.015
[140] Yu P, Chan K C, Xia L, et al. Enhancement of strength and corrosion resistance of copper wires by metallic glass coating [J]. Mater. Trans., 2009, 50: 2451
doi: 10.2320/matertrans.M2009157
[141] Meng Y J, Xi T, Yang C G, et al. Effect of gallium addition on mechanical and antibacterial properties of 304L stainless steel [J]. Acta Metall. Sin., 2024, 60: 890
doi: 10.11900/0412.1961.2022.00351
孟玉佳, 席 通, 杨春光 等. Ga添加对304L不锈钢力学性能和抗菌性能的影响 [J]. 金属学报, 2024, 60: 890
doi: 10.11900/0412.1961.2022.00351
[142] Mirshekari G R, Saatchi A, Kermanpur A, et al. Effect of post weld heat treatment on mechanical and corrosion behaviors of NiTi and stainless steel laser-welded wires [J]. J. Mater. Eng. Perform., 2016, 25: 2395
doi: 10.1007/s11665-016-2034-3
[143] Van Acker K, Root J, Van Houtte P, et al. Neutron diffraction measurement of the residual stress in the cementite and ferrite phases of cold-drawn steel wires [J]. Acta Mater., 1996, 44: 4039
doi: 10.1016/S1359-6454(96)00051-1
[144] Yang J W, Liu X Y, Li T, et al. Effect of Ni interlayer on microstructures and mechanical properties of 2205 duplex stainless steel joint by laser oscillating welding [J]. J. Iron Steel Res. Int., 2024, 31: 2463
doi: 10.1007/s42243-024-01328-w
[145] Peng Z X, Hu R Z, Liu J, et al. Probing local difference of martensite formation: A study on localized deformation modes in drawn 304H stainless steel wires [J]. J. Iron Steel Res. Int., 2025, 32: 991
doi: 10.1007/s42243-024-01308-0
[146] Wang F, Xiao G Z, Zou D N, et al. Effect of Nb on high-temperature oxidation of austenitic stainless steel at 850 oC [J]. J. Iron Steel Res. Int., 2025, 32: 1003
doi: 10.1007/s42243-024-01297-0
[147] Wang Y X, Gong W, Su Y H, et al. Application of neutron characterization techniques to metallic structural materials [J]. Acta Metall. Sin., 2024, 60: 1001
doi: 10.11900/0412.1961.2024.00063
王延绪, 龚 武, 苏玉华 等. 中子表征技术在金属结构材料研究中的应用 [J]. 金属学报, 2024, 60: 1001
doi: 10.11900/0412.1961.2024.00063
[148] Schajer G S. Relaxation methods for measuring residual stresses: Techniques and opportunities [J]. Exp. Mech., 2010, 50: 1117
doi: 10.1007/s11340-010-9386-7
[149] Isavand S, Assempour A. Strain localization and deformation behavior in ferrite-pearlite steel unraveled by high-resolution in-situ testing integrated with crystal plasticity simulations [J]. Int. J. Mech. Sci., 2021, 200: 106441
doi: 10.1016/j.ijmecsci.2021.106441
[150] Zhu L, Sun C Y, Wang B Y, et al. Cross wedge rolling deformation law and bonding mechanism of 304 stainless steel/Q235 carbon steel bimetallic shaft [J]. J. Iron Steel Res. Int., 2024, 31: 2423
doi: 10.1007/s42243-024-01300-8
[151] Peng X, Yao Q Z, Yi B, et al. Deep learning approach for predicting multi-component stress fields in fiber-reinforced composites under different load paths [J]. Compos. Sci. Technol., 2025, 267: 111198
doi: 10.1016/j.compscitech.2025.111198
[152] Li J Y, Zhang X Y, Shang C L, et al. Reinforcement learning in materials science: Recent advances, methodologies and applications [J]. Acta Metall. Sin. (Engl. Lett.), 2025, 38: 2077
doi: 10.1007/s40195-025-01934-x
[153] Yang P, Ye S W, Peng Y F. Three-dimensional profile stitching measurement for large aspheric surface during grinding process with sub-micron accuracy [J]. Precis. Eng., 2017, 47: 62
doi: 10.1016/j.precisioneng.2016.07.005
[154] Hu S Y, Ma X D, Zhang Y Q, et al. Application of self-supervised learning in steel surface defect detection [J]. J. Mater. Inf., 2025, 5: 44
[155] Song R X, Song G J. Metal Wire Woven Mesh Technology [M]. Beijing: Standards Press of China, 2007: 1
宋如轩, 宋国健. 金属丝编织网工艺学 [M]. 北京: 中国标准出版社, 2007: 1
[156] Yi J, Xia X X, Zhao D Q, et al. Micro- and nanoscale metallic glassy fibers [J]. Adv. Eng. Mater., 2010, 12: 1117
doi: 10.1002/adem.v12.11
[157] Zhang S H, Wang P, Li D Z, et al. Investigation of trip effect in ZG06Cr13Ni4Mo martensitic stainless steel by in situ synchrotron high energy X-ray diffraction [J]. Acta Metall. Sin., 2015, 51: 1306
张盛华, 王 培, 李殿中 等. ZG06Cr13Ni4Mo马氏体不锈钢中TRIP效应的同步辐射高能X射线原位研究 [J]. 金属学报, 2015, 51: 1306
[158] Meng Q K, Mei B Z, Zhang P, et al. In situ synchrotron X-ray diffraction study of deformation behavior of Ti39Nb alloy [J]. Chin. J. Nonferrous Met., 2022, 32: 845
孟庆坤, 梅碧舟, 张 盼 等. Ti-39Nb合金变形行为的原位同步辐射X射线衍射研究 [J]. 中国有色金属学报, 2022, 32: 845
[159] Wu S C, Xiao T Q, Withers P J. The imaging of failure in structural materials by synchrotron radiation X-ray microtomography [J]. Eng. Fract. Mech., 2017, 182: 127
doi: 10.1016/j.engfracmech.2017.07.027
[160] Guo E Y, Du Z L, Li B Z, et al. Research progress on magnesium alloys based on synchrotron radiation in situ characterization techniques [J]. Acta Metall. Sin., 2026, 62: 890
郭恩宇, 杜泽龙, 李炳志 等. 基于同步辐射原位表征技术的镁合金研究进展 [J]. 金属学报, 2026, 62: 890
doi: 10.11900/0412.1961.2025.00297
[161] Larson B C, Yang W G, Ice G E, et al. Three-dimensional X-ray structural microscopy with submicrometre resolution [J]. Nature, 2002, 415: 887
doi: 10.1038/415887a
[162] Schmidt S, Olsen U L, Poulsen H F, et al. Direct observation of 3-D grain growth in Al-0.1% Mn [J]. Scr. Mater., 2008, 59: 491
doi: 10.1016/j.scriptamat.2008.04.049
[163] Lodh A, Thool K, Samajdar I. X-ray diffraction for the determination of residual stress of crystalline material: An overview [J]. Trans. Indian Inst. Met., 2022, 75: 983
doi: 10.1007/s12666-022-02540-6
[164] Han J C, Song B, Xu P, et al. Multiscale synthesis and performance regulation mechanisms of high-entropy materials [J]. Acta Metall. Sin., 2026, 62: 397
doi: 10.11900/0412.1961.2025.00405
韩杰才, 宋 波, 徐 平 等. 高熵材料的多尺度制备及性能调控机制 [J]. 金属学报, 2026, 62: 397
doi: 10.11900/0412.1961.2025.00405
[165] Wu G L, Zhu W Q, He Q Y, et al. 2D and 3D orientation mapping in nanostructured metals: A review [J]. Nano Mater. Sci., 2020, 2: 50
[166] Zhu W Q, Wu G L, Godfrey A, et al. Five-parameter grain boundary character distribution of gold nanoparticles based on three dimensional orientation mapping in the TEM [J]. Scr. Mater., 2022, 214: 114677
doi: 10.1016/j.scriptamat.2022.114677
[167] Zhang Y B, Fan G H. Three-dimensional X-ray diffraction technique for metals science [J]. Mater. China, 2017, 36: 181
张玉彬, 范国华. 三维X射线衍射技术在金属材料研究中的应用 [J]. 中国材料进展, 2017, 36: 181
[168] He Q Y, Schmidt S, Zhu W Q, et al. 3D microscopy at the nanoscale reveals unexpected lattice rotations in deformed nickel [J]. Science, 2023, 382: 1065
doi: 10.1126/science.adj2522 pmid: 38033081
[169] Wei Y, Gault B, Varanasi R S, et al. Machine-learning-based atom probe crystallographic analysis [J]. Ultramicroscopy, 2018, 194: 15
doi: S0304-3991(18)30159-1 pmid: 30036832
[1] LI Ruixue, ZHOU Chenxi, YANG Huimin, YONG Xingyue, LIU Jingjun. Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater[J]. 金属学报, 2026, 62(7): 1273-1287.
[2] WANG Wei, ZHANG Yubo, ZHAO Yan, WANG Tongmin, LI Tingju. Influences of High-Entropy Alloy Particles on the Microstructure and Mechanical Properties of Selective Laser Melted Al12Si Alloy During Solution Treatment[J]. 金属学报, 2026, 62(6): 1009-1020.
[3] WANG Bin, ZHAO Peng, LIU Jiawei, ZHANG Chunbo, QIN Zhiwei, DONG Honggang, LI Peng. Effect of Heat Treatment on Microstructural Evolution and Mechanical Properties of Inertial Friction Welded Joints for FGH96 Superalloy[J]. 金属学报, 2026, 62(6): 1043-1058.
[4] WANG Mingfei, TAO Meiyue, GONG Chen, PENG Bo, LI Tingju, JIE Jinchuan. Microstructural Evolution and Strengthening Mechanisms of Cu-Ni-Si/1010 Steel Bimetallic Composites via Direct Annealing and Cold Rolling + Annealing[J]. 金属学报, 2026, 62(6): 1091-1104.
[5] XU Dingfeng, HAN Feiyang, JIANG Qicheng, WANG Huan, SHANG Liyuan, LU Yiping. Composition Design and Optimization of Microstructure and Properties for an AlCrFeCoNi Low-Expansion Alloy[J]. 金属学报, 2026, 62(6): 1021-1031.
[6] ZHU Siying, YI Min, GUO Wanlin. Topological Properties and Characteristics of Grain Boundary Structure in Metallic Materials[J]. 金属学报, 2026, 62(5): 705-720.
[7] LU Zhaoping, SHEN Yaozu, WANG Xianzhen, CHEN Qiang, TANG Jianguo, ZHANG Xiaobin, YU Yong, JIANG Suihe, LIU Xiongjun, WANG Hui, WU Yuan. High-Entropy Alloys in Extreme Environments: A Perspective on Advantages, Challenges, and Breakthroughs[J]. 金属学报, 2026, 62(5): 743-755.
[8] ZHENG Yufeng, SHEN Yunong. Research Status and Future Directions of Pure Mo and Mo-Based Biodegradable Metals[J]. 金属学报, 2026, 62(5): 905-922.
[9] FAN Xiaoguang, XIAO Yunteng, ZHAN Mei, MA Fei, GAO Pengfei, ZHENG Zebang, ZHANG Xin, SHAO Guangda, WU Yuming. Strain Path Effects in Metal Plastic Forming: Mechanisms, Characterization, and Application[J]. 金属学报, 2026, 62(5): 975-992.
[10] CHEN Guang, CHEN Fengrui, ZHU Demin, LI Guizhong, LI Luo, SONG Weidong, WANG Zite, XIANG Henggao, CHEN Yang, QI Zhixiang. Polysynthetic Twinned High-Performance TiAl Alloy with Ordered Structures of Functional Units[J]. 金属学报, 2026, 62(4): 541-549.
[11] XIE Hongji, LI Jiarong, LUO Yushi, ZHENG Sujie, LUO Kailun. Effect of Solidification Conditions on Microstructure Evolution in DD6 Single-Crystal Superalloy[J]. 金属学报, 2026, 62(4): 550-560.
[12] HAN Jiecai, SONG Bo, XU Ping, XU Yifei, WANG Kaixi. Multiscale Synthesis and Performance Regulation Mechanisms of High-Entropy Materials[J]. 金属学报, 2026, 62(3): 397-405.
[13] WANG Jianfeng, XU Zhenmu, LIU Zhan, GAO Zhuanni, ZHAN Xiaohong. Effect of Ultrasonic Vibration on the Microstructure and Strengthening Mechanism of Narrow Gap Laser Welding of TC4 Titanium Alloy[J]. 金属学报, 2026, 62(3): 406-420.
[14] JIANG Zhida, XU Yangyang, YU Jiaxin, LIU Wencai, ZHU Haowen, WU Guohua, SHANG Zhengping. Mechanical and Conductive Properties of Cu/1060Al/Cu Three-Layer Composite Prepared by High-Temperature Oxygen-Free Rolling[J]. 金属学报, 2026, 62(3): 431-444.
[15] CUI Tianliang, XIE Xingfei, WEN Xiaocan, LYU Shaomin, QU Jinglong, DU Jinhui. Tensile Behavior and Fracture Mechanism of Hard-to-Deform GH4151 Superalloy[J]. 金属学报, 2026, 62(3): 445-457.
No Suggested Reading articles found!