TiAl-BASED COMPOSITE SHEET WITH MULTI-LAYER DISTRIBUTED REINFORCEMENT PREPARED BY SOLID-LIQUID REACTION
CUI Xiping, GENG Lin, FANG Kun, FAN Guohua, ZHENG Zhenzhu, WANG Guisong
School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
Cite this article: 

CUI Xiping, GENG Lin, FANG Kun, FAN Guohua, ZHENG Zhenzhu, WANG Guisong. TiAl-BASED COMPOSITE SHEET WITH MULTI-LAYER DISTRIBUTED REINFORCEMENT PREPARED BY SOLID-LIQUID REACTION. Acta Metall Sin, 2013, 49(11): 1462-1466.

Download:  PDF(1836KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

TiAl-based alloy have potential as high temperature structural materials for aerospace applications, especially for thermal protection systems in aerospace vehicles including skin materials. Unfortunately, the ductility and formability of TiAl-based alloys are rather poor and thus γ-TiAl sheets or foils are quite difficult to be manufactured by traditional methods and still far from practical applications. In the present work, commercial pure Ti foils and in-house fabricated TiB2/Al composite foils were alternately stacked and rolled to prepare Ti-(TiB2/Al) laminates, and then heat treatment was utilized to make liquid Al react with solid Ti,and finally TiAl-based composite sheet with multi-layer distributed reinforcement TiB2 particles were achieved. This method avoided the direct deformation of brittle TiAl billets and thus the near-net-shape processing of TiAl-based alloys sheets was feasible. Phase transformation and microstructure evolution during heat treatment were investigated and mechanical properties of the resulting micro-laminated TiB2-TiAl composite sheets were evaluated. The results showed that porous TiAl3 layers were produced by the reaction between liquid Al and solid Ti because of Kirkendall effect, and the following densification treatment under 50 MPa at 1300℃ for 2 h significantly improved the relative density of material. Subsequently, the reaction diffusion between TiAl3 and residual Ti proceeded in the following heat treatment, and finally fully lamellar (α2-Ti3Al+γ-TiAl) layers were obtained. TiB2 particles did not participate in any reaction and remained, and displayed multi-layered distribution in the matrix(α2-Ti3Al+γ-TiAl) layers. TiB2-rich layer hindered the coarsening of lamellar colony of (α2-Ti3Al+γ-TiAl) layer. Tensile properties at 800℃ of multi-layered TiB2-TiAl composite sheets remarkably increased because of an increase of energy dissipation caused by plastic deformation.

Received:  04 September 2013     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2013.00546     OR     https://www.ams.org.cn/EN/Y2013/V49/I11/1462

[1] Zhong H, Yang Y L, Li J S, Wang J, Zhang T B, Li S, Zhang J.  Mater Lett, 2012; 83: 198

[2] Wu X H.  Intermetallics, 2006; 14: 1114
[3] Draper S L, Krause D, Lerch B, Locci I E, Doehnert B, Nigam R, Das G, Rissbacher K.Mater Sci Eng, 2007; A464: 330
[4] Liu R C, Wang Z, Liu D, Bai C G, Cui Y Y, Yang R.  Acta Metall Sin, 2013; 49: 642
(刘仁慈, 王震, 刘冬, 柏春光, 崔玉友, 杨锐.金属学报, 2013; 49: 642)
[5] David E A, Jeffrey A H.  JOM. 1994; 3: 31
[6] Fukutomi H, Ueno M, Nakamura M, Suzuki T, Kikuchi S.  Mater Trans JIM, 1999; 40: 654
[7] Luo J G, Acoff V L.  Mater Sci Eng, 2006; A433: 334
[8] Xu L, Cui Y Y, Hao Y L, Yang R.  Mater Sci Eng, 2006; A435-436: 638
[9] Jakob A, Speidel M O.  Mater Sci Eng, 1994; A189: 134
[10] Chaudhari G P, Acoff V L.  Intermetallics, 2010; 18: 472
[11]Shu S L, Xing B, Qiu F, Jin S B, Jiang Q C.  Mater Sci Eng, 2013; A560: 596
[12] Sun T, Wang Q, Sun D L, Wu G H, Na Y.  Wear, 2010; 268: 693
[13] Chaudhari G P, Acoff V L.  Compos Sci Technol, 2009; 69: 1667
[14] Yang R, Cui Y Y, Dong L M, Jia Q.  J Mater Process Technol, 2003; 135: 185
[15] Bravo P M, Madariaga I, Ostolaza K, Tello M.  Scr Mater, 2005; 53: 1142

[16] Wang J N, Xie K.  Scr Mater, 2000; 43: 442

No related articles found!
No Suggested Reading articles found!