Please wait a minute...
Acta Metall Sin  2011, Vol. 47 Issue (6): 706-712    DOI: 10.3724/SP.J.1037.2011.00012
论文 Current Issue | Archive | Adv Search |
NUMERICAL SIMULATION OF KEYHOLE SHAPE AND TRANSFORMATION FROM PARTIAL TO OPEN STATES IN PLASMA ARC WELDING
HUO Yushuang 1,2, WU Chuansong 1, CHEN Maoai 1
1. Key Lab for Solid–Liquid Structure Evolution and Materials Processing (Ministry of Education), Shandong University, Jinan 250061
2. School of Materials Science and Engineering, Shandong Jianzhu University, Jinan 250101
Cite this article: 

HUO Yushuang, WU Chuansong, CHEN Maoai. NUMERICAL SIMULATION OF KEYHOLE SHAPE AND TRANSFORMATION FROM PARTIAL TO OPEN STATES IN PLASMA ARC WELDING. Acta Metall Sin, 2011, 47(6): 706-712.

Download:  PDF(1265KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  It is of great significance to develop a mathematical model of keyhole shape and dimension in order to widen the process parameter window and improve the process stability in keyhole plasma arc welding (PAW). In this study, a keyhole model was developed according to the force–balance conditions on the keyhole wall. The establishing process of quasi–steady state keyhole was numerically simulated for stainless steel plates of 6 mm thickness, and the keyhole shapes and dimensions were obtained under different welding process parameters. The transformation mechanism of the keyhole from blind (partial) to open (complete) states in PAW process was analyzed based on the calculated action forces on the keyhole wall. The values of action forces at different locations on the keyhole wall were calculated. With increasing of welding current, the keyhole depth rised in a nonlinear way. There existed a critical value of welding current, i.e., if welding current was a little bit hgher than this value, the keyhole inside the weld pool would suddenly transform from partial state (blind keyhole) ino complete state (open keyhole). The fast centralization of the plasma arc force at the keyhole bottom region resulted in the sudden transformation from a partial keyhole to an open keyhole. The keyhole PAW experiments were conducted to validate the numerical analyss results.
Key words:  keyhole plasma arc welding      keyhole shapeforce–balance equation      numerical analysis     
Received:  07 January 2011     
ZTFLH: 

TG456.2

 
Fund: 

Supported by Key Project of National Natural Science Foundation of China (No.50936003)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2011.00012     OR     https://www.ams.org.cn/EN/Y2011/V47/I6/706

[1] Lucas W. In: Japan Welding Society ed., Proc 8th Int Welding Symposium, Osaka, Japan: Japan Welding Society, 2008: 189

[2] Zhang Y M, Zhang S B. Weld J, 1999; 75: 53s

[3] Wu C S, Jia C B, Chen M A. Weld J, 2010; 89: 225s

[4] Dong C L, Wu L, Shao Y C. China Mech Eng, 2000; 11: 577

(董春林, 吴林, 邵亦陈. 中国机械工程, 2000; 11: 577)

[5] Keanini R G, Rubinsky B. Int J Heat Mass Transfer, 1993; 36: 3283

[6] Fan H G, Kovacevic R. J Phys, 1999; 32D: 2902

[7] Li L, Hu S S. J Tianjin Univ, 2007; 40: 260

(李力, 胡绳荪. 天津大学学报, 2007; 40: 260)

[8] Metcalfe J C, Quigley M B C. Weld J, 1975; 54: 99s

[9] Wu C S, Hu Q X, Gao J Q. Comp Mater Sci, 2009; 46: 167

[10] Hu Q X, Wu C S, Zhang Y M. China Weld, 2007; 16: 55

[11] Huo Y S, Wu C S. China Weld, 2009; 18: 12

[12] Nehad A K. Int Comm Heat Mass Transfer, 1995; 22: 779

[13] Wang X J, Wu C S, Chen M A. Acta Metall Sin, 2010; 46: 984

(王小杰, 武传松, 陈茂爱. 金属学报, 2010; 46: 984)

[14] Toit M D, Pistorius P C. Weld J, 2007; 86: 222s

[15] Sahoo P, DebRoy T, McNallan M J. Metal Trans, 1988; 19B: 483
[1] Xue WANG,Lei HU,Dongxu CHEN,Songtao SUN,Liquan LI. Effect of Martensitic Transformation on Stress Evolution in Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes[J]. 金属学报, 2017, 53(7): 888-896.
[2] . NUMERICAL ANALYSIS OF TRANSIENT DEVELOPMENT OF TEMPERATURE FIELD IN KEYHOLE PLASMA ARC WELDING[J]. 金属学报, 2006, 42(3): 311-316 .
[3] WU Chuansong; CAO Zhenning; WU Lin (Harbin Institute of Technology). NUMERICAL ANALYSIS OF THREE-DIMENSIONAL FLUID FLOW AND HEAT TRANSFER IN TIG WELD POOL WITH FULL-PENETRATION[J]. 金属学报, 1992, 28(10): 47-52.
No Suggested Reading articles found!