| KINETICS OF THE LEACHING OF COPPER SLAG IN AMMONIA SOLUTION UNDER HIGH OXYGEN PRESSURE |
| Liu;S.P.;Chow;Y.H.and Shieh;N.T.Kunming Research Station of the Institute of Metallurgy and Ceramics;Academia Sinica |
|
Cite this article:
Liu;S.P.;Chow;Y.H.and Shieh;N.T.Kunming Research Station of the Institute of Metallurgy and Ceramics;Academia Sinica. KINETICS OF THE LEACHING OF COPPER SLAG IN AMMONIA SOLUTION UNDER HIGH OXYGEN PRESSURE. Acta Metall Sin, 1958, 3(2): 99-110.
|
|
|
Abstract The copper slag under investigation contains chiefly of metallic copper,matteand copper oxides.In order to dissolve both metallic and Cu_2S contained in matte,it is necessary to provide an oxidation condition for the leaching process in highpressure autoclave.The purpose of our investigation was:1.To study the kineticsof the leaching processes;2.To find the most efficient leaching conditions.The kinetics of the leaching process were investigated over a wide range ofNH_4OH and(NH_4)_2CO_3 concentrations,oxygen pressures,temperatures of the solu-tion and stirring velocities.The experimental results show that the leaching processes were diffusion con-trolled reactions,in other words,velocity of diffusion determines the over-all rateof the leaching process and by increasing the speed of agitation of the reactants,the % of Cu extraction is increased.All the experimental results show that the rate of leaching process obeys para-bolic law,that is,the % of copper extraction against time is parabolic functioThe parabolic constant K_P,and the slope of the parabolic were calculatedagainst velocities of stirring,oxygen pressures,concentrations of NH_4OH and(NH_4)_2CO_3and temperatures of the solution.The influence of pH values against the % of copper extraction is a straight-line relationship,but reaches a maximum at some definite pH value.The effect of temperatures upon the efficiency of copper extraction is alsostudied and the plot of log K_P against 1/T gives a straight line relationship.Theactivation energy of this diffusion controlled process was 3.1 kcal/mol.At 60℃,speed of stirring of 360 r.p.m.O_2-pressure of 5 atmospheres and0.65 N of NH_4OH+0.12 N of(NH_4)_2CO_3,the % of copper extraction of this slagwhich contained only 0.96% total copper,is 75% with a leaching time of 8 hours.
|
|
Received: 18 February 1958
|
[1] Paul H.Emmett,Catalysis,volume 1,Fundamental Principles(part 1) . [2] June F.Zimmerman,J.Phy.Chem.and Colli.,562(1949) . [3] J.Halpern,J.of the Elec.Chem.Soc.,100,№ 10,11(1953) . [4] Huber T.S.Brittos,Hydrogen Ions,(1955) . [5] #12 [6] Gunther Cohn,Chem.Reviews,42(1948) ,p.527. [7] Pauls,Roller,J.of Phy.Chem.,39(1935) ,P.221. [8] J.Halpern,Bulletin of the Inst.of Min.and Metal,№ 606,2(1957) . [9] #12 [10] John P.Baur.Donald W.,J.of the Elec.Chem.Soc.,102,№ 8(1955) . [11] R.W.Lane and H.J.McDonald,J.of Amer.Chem.Soc.,68-2(1946) . [12] #12$ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|