Abstract  By using the normal-pressure chlorine method in conjunction with the electrolytic method,the problem of the quantitative determination of non-metallic inclusions in low-chromium steelsand steels with carbon content more than 0.5% was successfully solved. With the arrangementand procedures being simplified, the low-pressure chlorine method has also been found successfulin the determination of non-metallic inclusions in ball-bearing steel. The practicability of ferrous-sulfate electrolytic method has been further comfirmed.
Received:  18 February 1959     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1959/V4/I2/162

[1] Colbeck E. W., Craven S. W., Murry W.: J. Iron & Steel Inst. 134 (1936 No.2) 251.
[2] Colbeck E. W., Craven S. W., Murry W.: Iron & Steel Inst. Special Report No.25 (1939) 109.
[3] Colbeck E. W., Craven S. W., Murry W.: J. Iron & Steel Inst. 143 (1941 No.1) 332.
[4] Colbeck E. W., Craven S. W.: J. Iron & Steel Inst. 148 (1943 No.2) 243.
[5] Klinger P. & Koch W.: Stahl u. Eisen 68 (1948) 321.
[6] Klinger P. & Koch W.: Beitrage zur metallkundlichen Analyse (1949) .
[7] 细田薰,桐野利定,田上豊助,东出秀雄;铁钢 42(1956) 901.
[8] Piper E., Hagedon H., Kern H., Ingeln J.: Radex Rundschan 5--6 (1957) 727.
[9] Koch W., Sundermann H.; Radex Rundschan 5--6 (1957) 679.
[10] Short C. W.. Roberts R. S., Croall G.; J. Iron & Steel Inst. 186 (1957) 85.
[11] Клячко Ю. А., Атласов А. Г., Шапиро М. М.; (1953) 352.
[12] 庄有智、白玉文、李静媛、李代锺;金属学报,第1卷第1期(1956) 59.
[13] 师昌绪、李代锺、赵淑熙;金属学报,第2卷第3期(1957) 295.
[14] 李代锺、赵淑熙、白玉文、师昌绪;钢铁工厂试验室,10(1958) 1.
No related articles found!
No Suggested Reading articles found!