| ON THE DETERMINATION OF NON-METALLIC INCLUSIONS IN LOW-CHROMIUM STEELS WITH CHLORINE METHODS |
| LEE TAI-CHUNG;CHAO SHU-HSI;LU TSIN-HUA Institute of Metal Research; Academia Sinica |
|
Cite this article:
LEE TAI-CHUNG;CHAO SHU-HSI;LU TSIN-HUA Institute of Metal Research; Academia Sinica. ON THE DETERMINATION OF NON-METALLIC INCLUSIONS IN LOW-CHROMIUM STEELS WITH CHLORINE METHODS. Acta Metall Sin, 1959, 4(2): 162-168.
|
|
|
Abstract By using the normal-pressure chlorine method in conjunction with the electrolytic method,the problem of the quantitative determination of non-metallic inclusions in low-chromium steelsand steels with carbon content more than 0.5% was successfully solved. With the arrangementand procedures being simplified, the low-pressure chlorine method has also been found successfulin the determination of non-metallic inclusions in ball-bearing steel. The practicability of ferrous-sulfate electrolytic method has been further comfirmed.
|
|
Received: 18 February 1959
|
[1] Colbeck E. W., Craven S. W., Murry W.: J. Iron & Steel Inst. 134 (1936 No.2) 251. [2] Colbeck E. W., Craven S. W., Murry W.: Iron & Steel Inst. Special Report No.25 (1939) 109. [3] Colbeck E. W., Craven S. W., Murry W.: J. Iron & Steel Inst. 143 (1941 No.1) 332. [4] Colbeck E. W., Craven S. W.: J. Iron & Steel Inst. 148 (1943 No.2) 243. [5] Klinger P. & Koch W.: Stahl u. Eisen 68 (1948) 321. [6] Klinger P. & Koch W.: Beitrage zur metallkundlichen Analyse (1949) . [7] 细田薰,桐野利定,田上豊助,东出秀雄;铁钢 42(1956) 901. [8] Piper E., Hagedon H., Kern H., Ingeln J.: Radex Rundschan 5--6 (1957) 727. [9] Koch W., Sundermann H.; Radex Rundschan 5--6 (1957) 679. [10] Short C. W.. Roberts R. S., Croall G.; J. Iron & Steel Inst. 186 (1957) 85. [11] Клячко Ю. А., Атласов А. Г., Шапиро М. М.; (1953) 352. [12] 庄有智、白玉文、李静媛、李代锺;金属学报,第1卷第1期(1956) 59. [13] 师昌绪、李代锺、赵淑熙;金属学报,第2卷第3期(1957) 295. [14] 李代锺、赵淑熙、白玉文、师昌绪;钢铁工厂试验室,10(1958) 1. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|