| STATISTICAL THEORY OF MOLTEN SALT SOLUTIONS Ⅲ. PHASE EQUILIBRIUM OF TERNARY HOMO-IONIC SYSTEMS |
| CH'N NIAN-YI; CHANG KUI-CH'NG (Instiute of Metallurgy; Academia Sinica) |
|
Cite this article:
CH'N NIAN-YI; CHANG KUI-CH'NG (Instiute of Metallurgy; Academia Sinica). STATISTICAL THEORY OF MOLTEN SALT SOLUTIONS Ⅲ. PHASE EQUILIBRIUM OF TERNARY HOMO-IONIC SYSTEMS. Acta Metall Sin, 1966, 9(2): 148-157.
|
|
|
Abstract From a statistical model of molten salt solutions, suggested in Part Ⅰ, two equations for the liquidus surfaces of the phase diagrams of AB-AC-AD and A_2B-AC-AD types were derived. The results of calculation were compared with the experimental data of many ternary phase diagrams, with good agreement, For the ternary homo-ionic Systems of other types, some relations between the geometric characteristics of the phase diagrams and the energetic parameters of solution were discussed.
|
|
Received: 18 February 1966
|
[1] 陈念贻、张桂成:金属学报,1964,7,12. [2] 陈念贻、张桂成:金属学报,1964,7,111. [3] Forland, T.: J. Phys. Chem., 1955, 59, 152. [4] #12 [5] #12 [6] #12 [7] #12 [8] #12 [9] #12 [10] #12 [11] #12 [12] #12 [13] #12 [14] #12 [15] #12 [16] #12 [17] #12 [18] #12 [19] #12 [20] #12 [21] #12 [22] #12 [23] #12 [24] #12 [25] #12 [26] #12 [27] #12 [28] #12 [29] #12 [30] 鲁日娜亚、徐晓白:化学学报,1958,24,356. [31] #12 [32] #12 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |