Please wait a minute...
Acta Metall Sin  1978, Vol. 14 Issue (3): 253-333    DOI:
Current Issue | Archive | Adv Search |
UNHEALED POROSITIES AND CRYSTALLINE STEPS IN FLAKES
Chen Lian Xu Yong-bo Yin Wan-quan(Institute of Metal Research; Academia Sinica)
Cite this article: 

Chen Lian Xu Yong-bo Yin Wan-quan(Institute of Metal Research; Academia Sinica). UNHEALED POROSITIES AND CRYSTALLINE STEPS IN FLAKES. Acta Metall Sin, 1978, 14(3): 253-333.

Download:  PDF(4487KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Dark seams along the rolling direction in certain cases could be observed by means of stereo-microscopic examination of flakes and under higher magnifications in a SEM. These seams were identified as unhealed porosities with crystalline steps and microholes on their inner free surface. The unhealed porosities might be a possible source of flake formation.
Received:  18 March 1978     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1978/V14/I3/253

[1] “层次结构”断口三结合研究组,金属学报,12(1976) ,92.
[2] Musatti, I. and Reggior, A., Metal Progr., 3 (1936) , 51.
[3] Scott, T. E. and Troiano, A. R., J. Metals, 11 (1959) , 619.
[4] Dana, A. W. et al., Trans. AIME, 7 (1955) , 895.
[5] #12
[6] 下川義雄,鉄鋼,57(1971) ,1992.
[7] Pittinato, G. F. et al., SEM/TEM Fractography Handbook, Metals and Ceramics Information Center, Columbus, (1975) , p. 56.
[8] ASM Metals Handbook, vol. 9, Fractography and Atlas of Fractography (1974) , p. 89.
[9] Engel-Klingele, Rasterelektronenmikroskopische Untersuchungen von Metallschaden, Gerling Institut fur Schadenforschung und Schadenverhutung GmbH, Koln (1974) , p. 114.
[10] Phillips, A. and Kerlins, V., Metal Progr., 95 (1969) , 81.
[11] Hemsworth, B. et al., Metal Constr. Brit. Weld. J., 1 (1969) , 5.
[12] Ryder, D. A., Acta Met., 9 (1961) , 73.
[13] 周敬等,金属学报,14(1978) .#
No related articles found!
No Suggested Reading articles found!