| COMPOSITE RECIPROCAL LATTICE UNIT CELLS FOR CUBIC TWINS |
| Liu Wen-xi |
|
Cite this article:
Liu Wen-xi. COMPOSITE RECIPROCAL LATTICE UNIT CELLS FOR CUBIC TWINS. Acta Metall Sin, 1978, 14(4): 397-408.
|
|
|
Abstract Hexagonal unit cells of composite reciprocal lattice have been derived for bcc as well as for fcc twin crystals, with these models, the characteristics of electron diffraction patterns of twinning in cubic systems can be figuratively described, thus simplifying the calculating and indexing processes of these patterns.
|
|
Received: 18 April 1978
|
[1] Pashley, D. W. and Stowell, M. J., Phil Mag., 8 (1963) , 1605. Hirsch. P. B. et al., Electron Microscopy of Thin Crystals, Butterworths, London, 1975, p. 145, [2] Edington, J. W., Electron Diffraction in the Electron Microscope, Philips, London and Basingstoke, 1975, p. 47. [3] 桶谷繁雄,電子線回折金属碳化物研究,東京,1971,p.69. [4] #12 [5] Kelly, P. M., Trans. AIME, 233 (1965) , 264. [6] Andrews, K. W. et al, Interpretation of Electron Diffraction Patterns, Hilger, London, 1971, p. 53. [7] 陈乾惕,金属学报,14(1978) ,428. [8] 电子衍射,中国科学院金属研究所技术资料,1976. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|