ON THE STABILITY OF BINARY COMPLEX OXIDES
Chen Nianyi;Wen Yuankai Shanghai Institute of Metallurgy; Academia Sinica University of Science and Technology of china
Cite this article: 

Chen Nianyi;Wen Yuankai Shanghai Institute of Metallurgy; Academia Sinica University of Science and Technology of china. ON THE STABILITY OF BINARY COMPLEX OXIDES. Acta Metall Sin, 1979, 15(1): 85-93.

Download:  PDF(479KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Factors concerning with the stability of binary complex oxides has been stu-died. For complex oxides with ionic bonds,the main factors determining the heatof formation of such oxides appear to be the relevant ionic radius and the va-lency of the component elements. For oxides with partial covalency, however, thescreening parameter proposed in this paper may also be important in addition tothe factors mentioned above.
Received:  18 January 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I1/85

[1] Erdos, E., Collect. Czech. Chem. Commun., 27 (1962) , 1428.
[2] Schwitzgebel, K. et al., J. Chem. Eng. Data, 16 (1971) , 418.
[3] Капустниский:络合物热化学(中译本),科学出版社,北京,1963.
[4] Thilo, E. et al., Z. Anorg. Allg. Chem., 303 (1960) , 90.
[5] 陈念贻,中国科学,(1974) ,№6,580;(1975) ,№ 4,399.
[6] 陈念贻,金属学报,11(1974) ,№ 2,154.
[7] 1963.
[8] 陈念贻,键参数函数及其应用,科学出版社,北京,1976.W
No related articles found!
No Suggested Reading articles found!