					Cite this article:
						|  |  
    					|  |  
    					| AN INVESTIGATION OF MAGNETIC Ni-Fe-Mo AND Ni-Fe-Nb ALLOYS |  
						| Xu Wenchong;Wang Junjian;Su Xiujin;Li Zhihua Beijing Institute of Iron and Steel Research |  
						|  |  
					
			      Xu Wenchong;Wang Junjian;Su Xiujin;Li Zhihua Beijing Institute of Iron and Steel Research. AN INVESTIGATION OF MAGNETIC Ni-Fe-Mo AND Ni-Fe-Nb ALLOYS. Acta Metall Sin, 1979, 15(2): 252-311.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  An investigation of the structures of Ni-Fe-Mo and Ni-Fe-Nb alloys has beencarried out by means of TEM supplemented by electron diffraction and X-ray dif-fraction analysis. The results obtained have been correlated with magnetic proper-ties as follows: Both alloys showed modulated structures, in which the Ni-Fe-Nb alloy beingcoarser and more predominant. As the proportion of modulated structures increases,the hardness of the alloy also increases, but vice versa in the case of its mag-netic permeability. The introduction of solute atoms Mo and Nb would lower the degree of or-dering in Ni_3Fe alloy, but fortunately only certain degree of ordering was sufficientto yield conditions for high permeability. A preprecipitating phase possessing thefcc (ordered) Ni_3Nb (γ′) structure and being coherent with the matrix,was observ-ed in the Ni-Fe-Nb alloy. This phase appears to promote the formation of modu-lated structures and exert a strengthening effect on matrix. |  
															| Received:  18 February 1979 |  
            
									            
									               
																												  
															| [1] Berkowitz, A. and Kweller, E., Magnetism and Metallurgy, Vol. 2, Academic, New York, 1969, p. 550. [2] Bozorth, R. M., Ferromagnetism, D. Van Nostrand Co., Toronto, 1953, p. 134.
 [3] 增本量,日本金属学会志,35(1971) ,985.
 [4] 比内正胜,日本金属学会志,40(1976) ,682.
 [5] Bourgeot, J., Mem. Sci. Rev. Met., 66 (1969) , 845.
 [6] 戴礼智,王俊健,侯德惠,金属学报,12(1976) ,102.
 [7] 郭可信,X射线学及电子显微术的进展,上海科技出版社,1966年,p.36.
 [8] 宫崎亨,日本金属学会会报,15(1976) ,309.
 |  
             
								                
															
																| 
																																																																									
																				| No Suggested Reading articles found! |  |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |