DETERMINATION OF THE ACTIVITY OF RE_2O_3 IN LIQUID RE_2O_3-CaF_2 AND RE_2O_3-CaO-CaF_2 SLAGS
Wang Changzhen;Yang Daiyin North-Eastern Institute of Technology
Cite this article: 

Wang Changzhen;Yang Daiyin North-Eastern Institute of Technology. DETERMINATION OF THE ACTIVITY OF RE_2O_3 IN LIQUID RE_2O_3-CaF_2 AND RE_2O_3-CaO-CaF_2 SLAGS. Acta Metall Sin, 1979, 15(3): 433-437.

Download:  PDF(299KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The activity of RE_2O_3 in both liquid RE_2O_3-CaF_2 and RE_2O_3-CaO-CaF_2 slagsat 1600℃ has been determined by equilibrating the slag with liquid tin in a gra-phite crucible under one atmosphere of carbon monoxide. Pure solid RE_2O_3 andpure liquid RE metals were chosen as the standard states and the equilibrium tem-perature was closely controlled to within ±2℃. The activity of RE_2O_3 in the re-action (RE_2O_3)+3C?2[RE]_(Sn)+3CO↑ was found to increase with the increase ofthe concentration of either RE_2O_3 in the RE_2O_3-CaF_2 system or RE_2O_3 and CaOin the RE_2O_3-CaO-CaF_2 system.
Received:  18 March 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I3/433

No related articles found!
No Suggested Reading articles found!