| ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-CaF_2 AND La_2O_3-CaF_2-CaO-SiO_2 SLAGS |
| Wang Changzhen;Zou Yuanxi (Chou Yuan-hsi) North-Eastern Polytechnical Institute Shanghai Institute of Metallurgy; Academia Sinica |
|
Cite this article:
Wang Changzhen;Zou Yuanxi (Chou Yuan-hsi) North-Eastern Polytechnical Institute Shanghai Institute of Metallurgy; Academia Sinica. ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-CaF_2 AND La_2O_3-CaF_2-CaO-SiO_2 SLAGS. Acta Metall Sin, 1980, 16(2): 190-194.
|
|
|
Abstract The activity of La_2O_3 in liquid La_2O_3-CaF_2 and La_2O_3-CaF_2-CaO-SiO_2 slagshas been determined at 1500℃ y equilibrating the slags with liquid tin in agraphite crucible under one atmosphere of carbon monoxide. From the ctivitydata on the La_2O_3-CaF_2 system, the activity of CaF_2 has been obtained by Gibbs-Duhem integration. The activity ata on the above mentioned slags are briefly discussed on thebasis of ionic constitution of liquid slags.
|
|
Received: 18 February 1980
|
[1] 王渭源,邹元爔,金属学报,6(1963) ,40. [2] 邹元爔,赵彭年,曹兆民,金属学报,6(1963) ,121. [3] Chou Yuan-hsi (邹元爔), Chow Ji-Cheng (周继程), Chao Peng-nian (赵彭年), Sci. Sinica, 12(1963) , 1249. [4] Chou Yuan-hsi (邹元爔), Chao Peng-nian (赵彭年), Sci. Sinica, 11 (1962) , 1287. [5] #12 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|