ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-CaF_2 AND La_2O_3-CaF_2-CaO-SiO_2 SLAGS
Wang Changzhen;Zou Yuanxi (Chou Yuan-hsi) North-Eastern Polytechnical Institute Shanghai Institute of Metallurgy; Academia Sinica
Cite this article: 

Wang Changzhen;Zou Yuanxi (Chou Yuan-hsi) North-Eastern Polytechnical Institute Shanghai Institute of Metallurgy; Academia Sinica. ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-CaF_2 AND La_2O_3-CaF_2-CaO-SiO_2 SLAGS. Acta Metall Sin, 1980, 16(2): 190-194.

Download:  PDF(369KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The activity of La_2O_3 in liquid La_2O_3-CaF_2 and La_2O_3-CaF_2-CaO-SiO_2 slagshas been determined at 1500℃ y equilibrating the slags with liquid tin in agraphite crucible under one atmosphere of carbon monoxide. From the ctivitydata on the La_2O_3-CaF_2 system, the activity of CaF_2 has been obtained by Gibbs-Duhem integration. The activity ata on the above mentioned slags are briefly discussed on thebasis of ionic constitution of liquid slags.
Received:  18 February 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I2/190

[1] 王渭源,邹元爔,金属学报,6(1963) ,40.
[2] 邹元爔,赵彭年,曹兆民,金属学报,6(1963) ,121.
[3] Chou Yuan-hsi (邹元爔), Chow Ji-Cheng (周继程), Chao Peng-nian (赵彭年), Sci. Sinica, 12(1963) , 1249.
[4] Chou Yuan-hsi (邹元爔), Chao Peng-nian (赵彭年), Sci. Sinica, 11 (1962) , 1287.
[5] #12
No related articles found!
No Suggested Reading articles found!