| LOW-FREQUENCY "AMPLITUDE PEAKS" IN THE INTERNAL FRICTION ASSOCIATED WITH THE INTERACTION OF SUBSTITUTIONAL SOLUTE ATOMS WITH DISLOCA-TIONS IN ALUMINIUM ALLOYS |
| Ge Tingsui (T. S. Kê) Institute of Metal Research; Academia Sinica |
|
Cite this article:
Ge Tingsui (T. S. Kê) Institute of Metal Research; Academia Sinica. LOW-FREQUENCY "AMPLITUDE PEAKS" IN THE INTERNAL FRICTION ASSOCIATED WITH THE INTERACTION OF SUBSTITUTIONAL SOLUTE ATOMS WITH DISLOCA-TIONS IN ALUMINIUM ALLOYS. Acta Metall Sin, 1980, 16(2): 218-230.
|
|
|
Abstract Low-frequency "amplitude peaks" and "temperature peaks" were observed inthe internal friction of dilute Al-Cu nd Al-Mg alloys around room temperature ata maximum surface-strain amplitude ranging from 5×10~(-7) to 1×10~(-5). This nom-alous internal friction showed a peculiar aging behaviour. An aging peak wasobserved in conjunction with the mplitude eak and the temperature peak. Suchpeaks have been observed repeatedly in: (1) heavily cold-worked specimens an-nealed ust rior to complete recrystallization; (2) fully annealed specimens cold-worked just after yielding; (3) fully annealed pecimens quenched from anelevated temperature. It is shown that the observed internal friction is associated with the nterac-tion of solute atoms (Cu and Mg in Al) with the mobile "fresh" dislocations pro-duced by cold-work or quenching. uch fresh dislocations contain a large numberof kinks. A modified dislocation atmosphere model was suggested in which thesolute atoms are assumed to be dragged along between two potential valleys dur-ing the to and fro sidewise motion of a ink under the action of the appliedalternating stress.
|
|
Received: 18 February 1980
|
[1] Ke,T.S.(葛庭燧),Phys.Rev.,76(1949) ,470. [2] Ke,T.S.(葛庭燧),Trans.AIME,188(1950) ,575. [3] Ke,T.S.(葛庭燧),Phys.Rev.,78(1950) ,420. [4] Ke,T.S.(葛庭燧),Science Record(科学记录),3(1950) ,61. [5] 葛庭燧,张进修,物理学报,21(1965) ,1711. [6] 葛庭燧,张进修,物理学报,22(1966) ,71. [7] 葛庭燧,张志舜,张进修,物理学报,22(1966) ,270. [8] 潘正良,王中光,孔庆虎,葛庭燧,待发表. [9] Seeger, A. and Schiller, P., Act. Met., 10 (1962) , 348. [10] Couch, W. E. and Swartz, J. E., Phil. Mag., 7 (1962) , 1231. [11] Perez, J., Peguin, P. and Gobin, P., Rev. Phys. Appl. 4 (1969) , 437. [12] Stadelmann, P. and Benoit, W., Internal Friction and Ultrasonic Attenuation in Solids, Ed. R. R. Hasiguti and N. Mikoshiba, University of Tokyo Press, 1977, p. 573, Fig. 2. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|