| STUDIES ON THE KINETICS OF Ni DISSOLUTION IN AQUEOUS AMMONIACAL SOLUTION |
| Xia Guangxiang;Chen Jiayong (Chen Chia-yung) Institute of Chemical Metallurgy; Academia Sinica |
|
Cite this article:
Xia Guangxiang;Chen Jiayong (Chen Chia-yung) Institute of Chemical Metallurgy; Academia Sinica. STUDIES ON THE KINETICS OF Ni DISSOLUTION IN AQUEOUS AMMONIACAL SOLUTION. Acta Metall Sin, 1980, 16(3): 290-301.
|
|
|
Abstract Studies have been carried out on the kinetics of Ni dissolution in aqueoussolution of NH_3 and (NH_4)_2CO_3 with O_2 present. It is shown that the NH_3 andNH_4~+ salt dissolution of Ni is an electrochemical reaction accompanied by surfaceoxidation of Ni by O_2. The reaction rate may be either in the NH_3 concentrationcontrol region or in the O_2 concentration control region depending on the ratio ofthe concentration of NH_3 and that of O_2. In the NH_3 controlling region, the surface of Ni will be passivated rathereasily with the formation of oxide film. The dissolution reaction will then beinterrupted. In the O_2 controlling region, the rate of reaction will be controlled bythe rate of O_2 transfer through the liquid film around the Ni surface. It can becorrelated with the equation of the rate of O_2 mass transfer.
|
|
Received: 18 March 1980
|
[1] Lane, R. W. and McDonald, H. J., J. Amer. Chem. Soc., 6B (1946) , 1699. [2] Benjamin, Lu. C. Y. and Graydon, W. F., ibid., 77 (1955) , 6136. [3] Halpern, J., J. Electrochem. Soc., 100 (1953) , 421. [4] Shimakage, K. and Morioka, S., Inst. Mining Met., Trans., C80 (1971) , 228. [5] 夏光祥,陈家镛,全国第一届冶金过程物理化学学术报告会论文集,上海科学技术出版社,1965,p.103. [6] Schlies, R. E. and Rarnsworth, H. E., Advan. Catal. Relat. Subj., 9 (1957) , 424. [7] Uhlig, H. H., Proceedings of the 3rd International Congress on Metallic Corrosion, Vol.1, 1966, 25. [8] Mellor, J. W., A Comprehensive Treatise on Inorganic and Theoretical Chemistry, Longmans, Green and Co., New York, Vol. 15, 1923, p. 152. [9] Chilton, T. H. and Colburn, A. P., Ind Eng. Chem., 26 (1934) , 1183. [10] Colburn, A. P., Trans. Amer. Inst. Chem. Eng., 29 (1933) , 174. [11] Eisenberg, M., Tobias, C. W. and Wilke, C. R., J. Electrochem. Soc., 101 (1954) , 306.? |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|