Please wait a minute...
Acta Metall Sin  1980, Vol. 16 Issue (3): 290-301    DOI:
Current Issue | Archive | Adv Search |
STUDIES ON THE KINETICS OF Ni DISSOLUTION IN AQUEOUS AMMONIACAL SOLUTION
Xia Guangxiang;Chen Jiayong (Chen Chia-yung) Institute of Chemical Metallurgy; Academia Sinica
Cite this article: 

Xia Guangxiang;Chen Jiayong (Chen Chia-yung) Institute of Chemical Metallurgy; Academia Sinica. STUDIES ON THE KINETICS OF Ni DISSOLUTION IN AQUEOUS AMMONIACAL SOLUTION. Acta Metall Sin, 1980, 16(3): 290-301.

Download:  PDF(919KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies have been carried out on the kinetics of Ni dissolution in aqueoussolution of NH_3 and (NH_4)_2CO_3 with O_2 present. It is shown that the NH_3 andNH_4~+ salt dissolution of Ni is an electrochemical reaction accompanied by surfaceoxidation of Ni by O_2. The reaction rate may be either in the NH_3 concentrationcontrol region or in the O_2 concentration control region depending on the ratio ofthe concentration of NH_3 and that of O_2. In the NH_3 controlling region, the surface of Ni will be passivated rathereasily with the formation of oxide film. The dissolution reaction will then beinterrupted. In the O_2 controlling region, the rate of reaction will be controlled bythe rate of O_2 transfer through the liquid film around the Ni surface. It can becorrelated with the equation of the rate of O_2 mass transfer.
Received:  18 March 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I3/290

[1] Lane, R. W. and McDonald, H. J., J. Amer. Chem. Soc., 6B (1946) , 1699.
[2] Benjamin, Lu. C. Y. and Graydon, W. F., ibid., 77 (1955) , 6136.
[3] Halpern, J., J. Electrochem. Soc., 100 (1953) , 421.
[4] Shimakage, K. and Morioka, S., Inst. Mining Met., Trans., C80 (1971) , 228.
[5] 夏光祥,陈家镛,全国第一届冶金过程物理化学学术报告会论文集,上海科学技术出版社,1965,p.103.
[6] Schlies, R. E. and Rarnsworth, H. E., Advan. Catal. Relat. Subj., 9 (1957) , 424.
[7] Uhlig, H. H., Proceedings of the 3rd International Congress on Metallic Corrosion, Vol.1, 1966, 25.
[8] Mellor, J. W., A Comprehensive Treatise on Inorganic and Theoretical Chemistry, Longmans, Green and Co., New York, Vol. 15, 1923, p. 152.
[9] Chilton, T. H. and Colburn, A. P., Ind Eng. Chem., 26 (1934) , 1183.
[10] Colburn, A. P., Trans. Amer. Inst. Chem. Eng., 29 (1933) , 174.
[11] Eisenberg, M., Tobias, C. W. and Wilke, C. R., J. Electrochem. Soc., 101 (1954) , 306.?
No related articles found!
No Suggested Reading articles found!