MICROSCOPIC IDENTIFICATION OF AIN
Zhang Detang
Cite this article: 

Zhang Detang. MICROSCOPIC IDENTIFICATION OF AIN. Acta Metall Sin, 1980, 16(3): 354-382.

Download:  PDF(2821KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A microscopic observation on AIN phase is made together with EPMA, X-rayor electron diffraction analysis. Its crystalline structure as well as chemical andmechanical properties are presented, and its original colour or optical feature isshown in colour photos.