RELATIONSHIP BETWEEN MECHANICAL PROPERTY OF METALS AND CRITICAL FRACTURE ANGLE OF A SLANTED CRACK
by Long Qiwei (Lung Chi-wei) (Institute of Metal Research; Academia Sinica)
Cite this article: 

by Long Qiwei (Lung Chi-wei) (Institute of Metal Research; Academia Sinica). RELATIONSHIP BETWEEN MECHANICAL PROPERTY OF METALS AND CRITICAL FRACTURE ANGLE OF A SLANTED CRACK. Acta Metall Sin, 1981, 17(3): 253-258.

Download:  PDF(470KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  New concept of two critical angles was suggested to fracture analysis of a slanted crack. A discussion was especially made of the material choice for small slant angle experiment. It is shown that all the metallic materials which used to be conventionally employed in such experiments seem to be not most satisfactory.
Received:  18 March 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I3/253

[1] 1976年北京断裂力学交流会第二次会议文集,1977,p.302,340.
[2] Hussain, M. A. Pu, S. L. and Underwood, J., Amer. Soc. Test. Mater., Spec. Tech. publ., № 560, 1973, p. 2.
[3] Hellen, T. K. and Blackburn, W. S., Int. J. Fracture, 11 (1975) , 605.
[4] 王仁东,1976年北京断裂力学交流会第二次会议论文集,1977,p.340.
[5] 高桦、王自强、杨成寿、周爱华,金属学报,15(1979) ,380.
[6] 龙期威,金属学报,12(1976) ,63.
[7] Lung Chi-Wei (龙期威), Preprint of the International Centre for Theoretical Physics, IC/79/72, 1979, Trieste Italy; Sci. Sinica, 23 (1980) , 441.
[8] Sih, G. C. and Macdonald, B., Eng. Fract. Mech., 6 (1974) , 361.
[9] Williams, J. G. and Ewing, P. D., Int. J. Fract. Mech. 8 (1972) , 441.
[10] Shah, R. C., Amer. Soc. Test. Mater., Spec. Tech. Publ., № 560, 1973, p. 29.
[11] 金属研究所,冶金系统第一届断裂韧性工作经验交流会资料选编,冶金部情报标准研究所,1976,p.132.
[12] 东北工学院,铸铁及其熔化,冶金工业出版社,1978,p.49.
[13] Marshall, G. P., Coutts, L. H. and Williams, J. G., J. Mat. Sci., 9 (1974) , 1409.
[14] Damage Tolerant Desigh Handbook, (MCIC-HB-01) , Columbus, Ohio. 1973.
[15] Knott, J. F., Fuodamentals of Fracture Mechanics, Butterworths, London, 1973, p. 112.
No related articles found!
No Suggested Reading articles found!