|
|
|
| CORRELATION BETWEEN NUMERAL FRACTURE CHAR-ACTERISTICS AND FRACTURE TOUGHNESS OF MEDIUM-CARBON CrNiMo STEEL |
| by Zhang Zhenfang; Zhang Tianyi and Liu Minzhi(Institute of Metal Research; Academia Sinica) |
|
Cite this article:
by Zhang Zhenfang; Zhang Tianyi and Liu Minzhi(Institute of Metal Research; Academia Sinica). CORRELATION BETWEEN NUMERAL FRACTURE CHAR-ACTERISTICS AND FRACTURE TOUGHNESS OF MEDIUM-CARBON CrNiMo STEEL. Acta Metall Sin, 1981, 17(3): 271-372.
|
|
|
Abstract An investigation was conducted to observe the microstructure and macro-or micro-fracture surface, and to determine the fracture toughness and impact toughness of fatigue precracked specimens of four different types of structure of a medium-carbon CrNiMo steel. Some primary results were shown that its highest fracture toughness was evaluated by the specimens of sorbitie structure tempered at 600℃, but the lowest up to about 300℃. An identical variation is noted between the impact toughness of the fatigue precracked specimens and the fracture toughness from tri-point bending tests. Moreover, the numeral estimation for the various fractured surface characteristics with relation to fracture toughness has been attempted.
|
|
Received: 18 March 1981
|
[1] Knott, J. F., Fundamentals of Fracture Mechanics, Butterworths, London, 1973, p. 114. [2] 小寺沢良一,金属材料,16(1976) ,№ 10,114. [3] Brothers, A. J., Hill, M., Parker, M. T., Spitzig, W. A., WieBe, W., and Wolff, U. F., Amer. Soc, Test. Mater., Spec. Tech. Publ. № 493, 1971, p. 3. [4] Wolff, U. E., Amer. Soc. Test. Mater., Spec. Tech. Publ. № 493, 1971, p. 20. [5] 大谷泰夫,寺崎富长久,邦武立郎,铁鋼,58(1972) ,434. [6] 寺崎富久长,大谷泰夫,铁鋼,58(1972) ,1067. [7] Gerberich, W. W. and Hartbower, C. E., ASM Trans. Quart., 61 (1968) , 184. [8] Bates, R. C. and Clark, W. G. Jr., ASM Trans. Quart., 62 (1969) , 380. [9] 西安交通大学金属材料及强度研究室,西安交通大学学报,1977,№ 4,49. [10] 西安交通大学金属材料及强度研究室,西安交通大学学报,1977,№ 4,35. [11] Kobayashi, H., Nakazawa, H. and Nakajima, A., Strength and Structure of Solid Materials, Leyden Noordhoff, 1976, pp. 115-128. [12] 陈篪,金属学报,13(1977) ,57. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|