| A CRITERION OF THE FORMATION OF AMORPHOUS STATE BY MELT QUENCHING |
| by Ning Yuantao and Zhou Xinming (Institute of Precious Metals Research) |
|
Cite this article:
by Ning Yuantao and Zhou Xinming (Institute of Precious Metals Research). A CRITERION OF THE FORMATION OF AMORPHOUS STATE BY MELT QUENCHING. Acta Metall Sin, 1981, 17(3): 278-284.
|
|
|
Abstract A criterion of the formation of amorphous state alloys by melt quenching has been proposed as I/ΔS<0.032 and (Ⅰ—0.1)/Δ>0.0044, where Ⅰ=1—T_m/T_m and S=1/100C_B((?)_m-T_m), T_m=melting point of the alloy, (?)_m=weighted average melting points of its components and C_B=at% of solute B. However, this criterion seems to be more accurate since special account has been taken of the effects of alloy composition and intermediate phase. All 127 alloys with one exception only checked up well with the criterion. Furthermore, the concentration distribution of the amorphous alloys and the characteristics of the allied constitution diagrams have been discussed.
|
|
Received: 18 March 1981
|
[1] Donald, I. W. and Davies, H. A., J. Non-Cryst. Solids, 30 (1978) , 77. [2] 施天生、郑如龙、陈念贻,金属学报,15(1979) ,94. [3] Anantharaman, T. R. and Suryanarayana, C., J. Mater. Sci., 6 (1971) , 1111. [4] Chen, H. S. and Jackson, K. A., Metallic Glasses, Papers Presented at a Seminar of the Materials Science Division of the ASM, Sept. 1976, ASM, Metals Park, Ohio, 1978, p. 74. [5] Sommer, F., Duddek, G. und Predel, B., Z. Metallk., 69 (1978) , 587. [6] Rapp, O., Lindberg, B., Chen, H. S. and Ran, K. V., J. Less-Common Metals, 62 (1978) , 221. [7] Duwez, P. and Johnson, W. L., J. Less-Common Metals, 62 (1978) , 215. [8] Anantharaman, T. R., Ramachandrarao, P., Suryanarayana, C., Lelc, S., Chattopadhyay, K., Sastry, G. V. S. and Davies, H. A., Rapidly Quenched Metal Ⅲ, Vol. 1, ed. by B. Cantor, London, 1978. [9] Chen, H. S. and Miller, C. E., Rev. Sci. Instrum., 41 (1970) , 1237. [10] Hansen, M., Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958. [11] Elliott, R. P., Constitution of Binary Alloys, First Suppl. McGraw-Hill, New York, 1965. [12] Hawkins, D. T. and Hultgren, R., Metals Handbook, 8th Ed., Vol. 8: Metallography Structures and Phase Diagrams, ASM, Metals Park, Ohio, 1973. [13] Takayama, S., J. Mater. Sci., 11 (1976) , 164. [14] Zielinski, P. G. and Matyja, H., Rapidly Quenched Metal Ⅱ, Section 1, ed. by N. J. Grant, B. C. Giesen, USA, MIT, 1976, p. 237. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|