Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (6): 677-681    DOI:
Current Issue | Archive | Adv Search |
AN INVESTIGATION OF THE PLASTIC ZONE IN THE VICINITY OF THE CRACK-TIP BY POSITRON ANNIHILATION TECHNIQUE
Ji Guokun; Liu Nianqing and Wang Shuying (Institute of High Energy Physics; Academia Sinica) and Jiang Jian; Xiong Liangyue and Long Qiwei (Institute of Solid State Physics; Academia Sinica; are now in the Institute of Metal Research; Academia Sinica)
Cite this article: 

Ji Guokun; Liu Nianqing and Wang Shuying (Institute of High Energy Physics; Academia Sinica) and Jiang Jian; Xiong Liangyue and Long Qiwei (Institute of Solid State Physics; Academia Sinica; are now in the Institute of Metal Research; Academia Sinica). AN INVESTIGATION OF THE PLASTIC ZONE IN THE VICINITY OF THE CRACK-TIP BY POSITRON ANNIHILATION TECHNIQUE. Acta Metall Sin, 1981, 17(6): 677-681.

Download:  PDF(371KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Central cracked and single edge cracked α-Ti specimens were loaded up to different stress levels and cut into four test pieces after unloading. Both parameters, positron lifetime and Doppler broadening lineshape S parameters were measured in the plastic zone at the crack tip. The Doppler broadening lineshape S parameters were measured as a function of distance from the crack tip along the crack direction, It was found that the S parameters decrease monotonically along the crack direction until the boundary of the plastic zone is reached. The size of plastic zone estimated by the positron annihilation method seems to agree roughly with that obtained from that calculated by fracture mechanics.
Received:  18 June 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I6/677

[1] Tanigawa, S. and Doyama, M., Progress in the Study of Application of Electron Theory to Materials Science. Ed. by M. Dovama. Univ. Tokyo. 1979. p. 1.
[2] 张天保,刘年庆,未发表资料.
[3] Wang, Y. Y. (王蕴玉), Chang, T, B. (张天保) and Wang, S. Y. (王淑英), Positron Annihilation, Proc. 5th Int. conf, on Positron Annihilation, Jpn. 1979, Ed. by R. R. Hashiguti and K. Pujiwara. Jpn. Inst. Met.. 1979. p. 227.
[4] 王淑英,未发表资料.
[5] Doyama, M., Progress in the Study of Point Defect, Ed. by M. Doyama, and S. Yoshids, Univ. Tokyo, 1977, p. 3.
[6] 陈篪等,金属断裂研究论文集,冶金工业出版社,1978,p.30.
[7] Brown, W. F. Jr.and Srawley, J.E., Am. Soc. Test. Mater., Spec. Tech. Publ., No. 410, 1967.
[8] Lardncr, R. W., Mathematical Theory of Dislocations and Fracture, Univ. Toronto, 1974, p. 163.
[9] Karras, M., Positron Annihilation, Proc. 5th Int. Conf. on Positron Annihilation, Jpn. 1979, Ed.. by R. R. Hashiguti, and K. Fujiwara, Jpn. Inst. Met., 1979, p. 257
No related articles found!
No Suggested Reading articles found!