A NEW INDEXING METHOD FOR HIGH ORDER LAUE POINTS
Zhao Chang'an (Nei Monggol Institute of Metallic Material Research)
Cite this article: 

Zhao Chang'an (Nei Monggol Institute of Metallic Material Research). A NEW INDEXING METHOD FOR HIGH ORDER LAUE POINTS. Acta Metall Sin, 1981, 17(6): 682-686.