Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (4): 425-432    DOI:
Current Issue | Archive | Adv Search |
ROLE OF NITROGEN IN GRAIN ORIENTED SILICON STEEL CONTAINING Al
Luo Yang Li Weili Chen Minqin Chen Minghao (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 19 February; 1981; revised manuscript 1 August; 1981)
Cite this article: 

Luo Yang Li Weili Chen Minqin Chen Minghao (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 19 February; 1981; revised manuscript 1 August; 1981). ROLE OF NITROGEN IN GRAIN ORIENTED SILICON STEEL CONTAINING Al. Acta Metall Sin, 1982, 18(4): 425-432.

Download:  PDF(732KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An attempt was made to understand the behaviour of Al and N, and to determine the mutual proper range of them contained in the grain oriented silicon steel. It has been shown that its magnetic properties is affected by the formation of AIN as effective inhibitor in which the N content seems to play an important role. The N both contained in solid solution and combined in AIN were determined by hydrogen extracting method. Finally, its technological feature influenced mainly by such AIN inhibitor has been discussed.
Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/425

1 Goss, N.P., Ind. Heat., 32(1965) , 1856.
2 Taguchi, S.; Yamamoto, T.; Sakakura, A., IEEE Trans. Magn., MAG-10(1974) , 123.
3 Goto, L; Matoba, L; Imanaka, T.; Gotoh, T.; Kan, T., Proceedings of the EPS Conference on Soft Magnetic Materials, University College, Cardiff, Wales, 1975, Vol. 2, p. 262.
4 Fiedler, H.C., IEEE Trams. Magn., MAG-13(1977) , 1433.
5 北京钢铁研究院硅钢组,金属学报,13(1977) ,80.
6 罗阳;李伟立;李玉凤;陈敏勤;陈易之,金属学报,17(1981) ,243.
7 陈名浩;张代仁,氢抽取法测定硅钢中固溶氮和有效粒度氮化铝,1979,待发表.
8 孙天锡;于宝文,工业生产Hi-B硅钢各工序显微组织及第二相有利夹杂的电镜研究,1980,待发表.<