Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (4): 463-471    DOI:
Current Issue | Archive | Adv Search |
FLOTATION OF SPODUMENE AND ITS SEPARATION FROM BERYL IN FROTH
Zhou Weizhi (Guangzhau Institute of Non-Ferrous Metals Research; Ministry of Metallurgical Industry) (Manuscript received 15 December; 1980)
Cite this article: 

Zhou Weizhi (Guangzhau Institute of Non-Ferrous Metals Research; Ministry of Metallurgical Industry) (Manuscript received 15 December; 1980). FLOTATION OF SPODUMENE AND ITS SEPARATION FROM BERYL IN FROTH. Acta Metall Sin, 1982, 18(4): 463-471.

Download:  PDF(608KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The flowsheet to float spodumene in alkaline medium without desliming has long since been borne out by its simplicity, low cost and easy supply of reagents. It was ensured in industrial practice that the spodumene concentrate with a grade of 6.0-6.1% Li_2O and recovery of 88-90% may be produced from ore containing 1.2-1.3% Li_2O. Several trials have been made to troubleshoot for separation of spodumene from the froth together with beryl such as:1050℃ decrepitating-sizing;600℃ roasting-flotation;85℃ digesting-flotation as well as flotation at room tem-perature. Among these the satisfactory results were obtained, and some of them were brought into operation in mills. Especially, the separation of beryl from spod-umene by flotation with“mixed reagent”(FeCl_3+Na_3SiO_3)add edto Na_2CO_3, Na_2S, oxidized paraffin soap at room temperature was a great success. Hence, the flowsheet of cleaning separation and bulk flotation of beryl-spodumene is developed providing a new way for recovery and separation of oughing froth containing these two minerals.
Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/463

1 Manser, R.M., Handbook of Silicate Flotation, Corwn Copyright, 1975, p. 94-101
2 周维志,金属学报,16(1980) ,249.
No related articles found!
No Suggested Reading articles found!