| CALCULATIONAL FORMULATION FOR VOLUME PERCENT OF γ′-PHASE IN PRECIPITATION HARDENING Ni-BASE SUPERALLOYS |
| YANG Hongcai (Northeast Institute of Technology; Shenyang) |
|
Cite this article:
YANG Hongcai (Northeast Institute of Technology; Shenyang). CALCULATIONAL FORMULATION FOR VOLUME PERCENT OF γ′-PHASE IN PRECIPITATION HARDENING Ni-BASE SUPERALLOYS. Acta Metall Sin, 1983, 19(2): 134-138.
|
|
|
Abstract A calculational formulation for v.-%, f, of γ′-phase in the precipitation hardening Ni-base superalloys was proposed as:where C denotes each wt-% of its own alloying element. It is available from the data obtained by chemical analysis. The abovementioned formulation was verified by about 20 commercial superalloys.
|
|
Received: 18 February 1983
|
1 杨洪才,金属学报,18(1982) ,511. 2 Dreshfleld, R. L.; Wallace, J. F., NASA-CR-120 940, (1972) . 3 高温合金金相图谱,冶金工业出版社,1979,p.25. 4 Decker, R. F.; Sims, C. T., The Superalloys, Eds. Sims, C. T.; Hagel, W. C., Wiley, New-York, 1972, p. 43. 5 高温合金--冶金学与生产,上海科学技术文献出版社,1980,p.126._ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|