ON THE TEMPERATURE DEPENDENCE OF CLEAVAGE FRACTURE TOUGHNESS OF SILICON STEEL
by DU Wanquan; CAI Qigong; LUO Ligeng (Central Iron and Steer Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 3 July; 1982; revised manuscript 6 December; 1982)
Cite this article:
by DU Wanquan; CAI Qigong; LUO Ligeng (Central Iron and Steer Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 3 July; 1982; revised manuscript 6 December; 1982). ON THE TEMPERATURE DEPENDENCE OF CLEAVAGE FRACTURE TOUGHNESS OF SILICON STEEL. Acta Metall Sin, 1983, 19(4): 71-79.
Abstract Results of experiments indicated that the analysis of the cleavage fracture of silicon steel seems to be hard to solve by RKR model. The Weibull statistical theory was introduced to describe the volume effect of the cleavage fracture stress determined by smooth tensile and notched bend specimens. The temperature dependence of the cleavage fracture toughness and its scatter band of silicon steel is formulated by applying the HRR theory and the Rice-Johnson's stress analysis for the blunted crack tip zone, as well as by combining with the Weibull's statistical model. The experimental data are in agreement with the prediction.
1 Ritchie, R. O.; Knott, J. F.; Rice, J. R., J. Mech. Phys. Solids, 21 (1973) , 395. 2 Pineau, A., Advances in Fracture Research, Vol. 2, Ed. Francois, D., Pergamon Press, 1981, p. 553. 3 Griffiths, J. R.; Owen, D. R. J. J. Mech. Phys. Solids, 19 (1971) , 419. 4 杜万泉,冶金部钢铁研究总院研究生毕业论文,1982. 5 Hutchinson, J. W., J. Mech. Phys. Solids, 16 (1968) , 13. 6 Tracey, D. M., J. Eng, Mater. Tech., 98 (1976) , 146. 7 陈箎;蔡其巩;王仁智,工程断裂力学(上)国防工业出版社,1978,p.77. 8 Rice, J. R.; Johnson, M. A., Inelastic Behavior of Solids, McGraw-Hill, New York, 1970, p.641.E