AN INVESTIGATION OF DYNAMIC RECRYSTALLI-ZATION OF TC6 Ti ALLOY
ZHANG Zhifang (Institute of Aeronautical Materials; Beijing); YUAN Zhenyi; TIAN Changsheng (North-West Engineering Institute Xi'an)
Cite this article:
ZHANG Zhifang (Institute of Aeronautical Materials; Beijing); YUAN Zhenyi; TIAN Changsheng (North-West Engineering Institute Xi'an). AN INVESTIGATION OF DYNAMIC RECRYSTALLI-ZATION OF TC6 Ti ALLOY. Acta Metall Sin, 1983, 19(5): 33-153.
Abstract An investigation was made of the dynamic recrystallization of TC6 Ti alloy by optical microscope and TEM. The three-dimensional dynamic recrystallization diagram of the alloy was establisbed and the optimum hot-deformation parameters for a uniform and fine size grain were determined. An discussion on the experimental results together with the static recrystallization theory is described.
1 Mcqueen, H. J.,高温形变时的回复和再结晶,中国科学院金属研究所,1981. 2 Chandra, T.; Weiss, I., Met. Sci., 16 (1982) , 97. 3 1980. 4 Verhoeven, J. D., Fundamentals of Physical Metallurgy, Wiley, New York, 1975, p.345. 5 Verhoeven, J. D., ibid., p.347. 6 Verhoeven, J.D., ibid., p.208. 7 刘云旭,金属热处理原理,机械工业出版社,1981,p.29.