Acta Metall Sin  1983, Vol. 19 Issue (5): 33-153    DOI:
Current Issue | Archive | Adv Search |
AN INVESTIGATION OF DYNAMIC RECRYSTALLI-ZATION OF TC6 Ti ALLOY
ZHANG Zhifang (Institute of Aeronautical Materials; Beijing); YUAN Zhenyi; TIAN Changsheng (North-West Engineering Institute Xi'an)
Cite this article: 

ZHANG Zhifang (Institute of Aeronautical Materials; Beijing); YUAN Zhenyi; TIAN Changsheng (North-West Engineering Institute Xi'an). AN INVESTIGATION OF DYNAMIC RECRYSTALLI-ZATION OF TC6 Ti ALLOY. Acta Metall Sin, 1983, 19(5): 33-153.

Download:  PDF(2073KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An investigation was made of the dynamic recrystallization of TC6 Ti alloy by optical microscope and TEM. The three-dimensional dynamic recrystallization diagram of the alloy was establisbed and the optimum hot-deformation parameters for a uniform and fine size grain were determined. An discussion on the experimental results together with the static recrystallization theory is described.
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/33

1 Mcqueen, H. J.,高温形变时的回复和再结晶,中国科学院金属研究所,1981.
2 Chandra, T.; Weiss, I., Met. Sci., 16 (1982) , 97.
3 1980.
4 Verhoeven, J. D., Fundamentals of Physical Metallurgy, Wiley, New York, 1975, p.345.
5 Verhoeven, J. D., ibid., p.347.
6 Verhoeven, J.D., ibid., p.208.
7 刘云旭,金属热处理原理,机械工业出版社,1981,p.29.
No related articles found!
No Suggested Reading articles found!