INFLUENCE OF RE ADDITION ON GRAIN GROWTH OFα-Al_2O_3 LAYER ON Fe-Cr-Al ALLOY
by LIBei; YAN Yuxin (Baotou Research Institute of Metallurgy; Nei Monggol)(Manuscript received 1 July; 1980; revised manuscript 1 August; 1983)
Cite this article: 

by LIBei; YAN Yuxin (Baotou Research Institute of Metallurgy; Nei Monggol)(Manuscript received 1 July; 1980; revised manuscript 1 August; 1983). INFLUENCE OF RE ADDITION ON GRAIN GROWTH OFα-Al_2O_3 LAYER ON Fe-Cr-Al ALLOY. Acta Metall Sin, 1984, 20(2): 143-220.

Download:  PDF(2475KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  When the Fe-23Cr-6Al alloy is under oxidation at 1300℃, the α-Al_2O_3 grains of single layer are formed initially as columnar crystals, and then, their columnar feature degenerated progressively owing to the columnar grains growing along transverse direction and the development of outer layer oxide consisted of equiaxial crystals. If the RE added, the growth rate of columnar grain along longitudinal direction is increased and along transverse direction decreased, as well as the growth rate of equiaxial grain of outer layer oxide also decreased. Consequently, their columnar feature become more intensive. For the alloy without RE, more crystalline whiskers and fine crystals are found on the surface of oxide layer. It may be considered that the Al ions diffusion through α-Al_2O_3 layer outwards is prevented by RE addition, and the oxide layer adherence is then improved.
Received:  18 February 1984     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I2/143

1 李碚;骆继群,金属学报,16(1980) ,401.
2 Golightly, F. A.; Stott, F. H.; Wood, G. C., Oxid. Met., 10 (1976) , 163.
3 Giggins, C. S.; Pettit, F, S., PWA Rep. 5364, (1975) .
4 李碚;骆继群;于洪香,钢铁,16(1981) ,№9,44.
5 Mistier, R. E.; Coble, R. L., J. Am. Ceram. Soc., 54(1971) , 60.
6 永井宏;村井照幸;三谷裕康,日本金属学会志,42(1978) ,1138.
7 Felten, E. J., J. Electrochem. Soc., 108(1961) , 490.
8 张立新;骆继勋;银耀德;李黎光;赵齐;张家芸,金属学报,17(1981) ,233.
No related articles found!
No Suggested Reading articles found!