Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (2): 182-187    DOI:
Current Issue | Archive | Adv Search |
PREFERENTIAL SPUTTERING ON THE SURFACE OF Ag-Pd ALLOY
by DONG Shuzhong; PANG Yanwan; DENG Jingfa; ZHU Xiaozhong(Fudan University; Shanghai)(Manuscript received 29 November; 1982; revised manuscript 9 May; 1983)
Cite this article: 

by DONG Shuzhong; PANG Yanwan; DENG Jingfa; ZHU Xiaozhong(Fudan University; Shanghai)(Manuscript received 29 November; 1982; revised manuscript 9 May; 1983). PREFERENTIAL SPUTTERING ON THE SURFACE OF Ag-Pd ALLOY. Acta Metall Sin, 1984, 20(2): 182-187.

Download:  PDF(504KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Changes in the surface composition of Ag-Pd alloy under argon ion bombardment have been monitored by XPS. It is shown that the surface of the alloy isrich in Ag after annealing and is rich in Pd after ion bombardment due to their different surface binding energy. The component sputtering yield ratio S_(Ag)/S_(Pd) is obtained using Shimizu model. The experiment and its results are compared with that obtained by the other researchers. It is found that the yield ratio varies with the alloy composition, and is related to the disorder surface layer formed by argon ion bombardment. The yield ratio S_(Ag)/S_(Pd) of the Pd dilute alloy (X_(Pd)=0.32 at.-%) is much larger than that of the others.
Received:  18 February 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I2/182

1 Sigmund, F., Sputtering by Particle Bombardment I, Ed. Behrisch, R., Sprlnger-Verlag, Berlin, 1981, p. 60.
2 Coburn, J. W., J. Vac. Sci. Technol., 13(1976) , 1037.
3 Braun, P.; Farber, W., Surf. Sci., 47(1975) , 57.
4 Okutani, T.; Shikata, M.; Shimizu, R., Surf. Sci., 99(1980) , 1410.
5 Frankenthal, R. P.; Siconolfi, D. L., ibid., 104(1981) , 205.
6 Zalar, A., Proc. of the 4th Int. Conf. on Solid Surface and the 3rd Europ. Conf. on Surface Science, Eds. Degras, D. A.; Costa, M., Supplement a la Revue, "Le Vide, les Couches Minces" n°201, 1980, p. 1311.
7 Mathieu, H. I.; Landolt, D., Surf. Sci., 53 (1975) , 228.
8 Garbassi, F.; Parravano, G., ibid., 71 (1978) , 42.
9 Slusser, G. I.; Winnograd, N., ibid., 84(1979) , 211.
10 Betz, G. Opitz, M.; Braun, P., Nucl. Instrum. Methods, 182/183(1981) , 63.
11 Mathieu, H. J.; Landolt, D., Proc. of the 4th Int. Conf. on Solid Surface and the 3rd Europ. Conf. on Surface Science, Eds. Degras, D. A.; Costa, M., Supplement a la Revue, "Le Vide, les Couches Minces" n°201, 1980, p. 1319.
12 Kuijers, F. J.; Pones, V., J. Catal., 60 (1979) , 100.
13 Shimizu, M.; Ono, M.; Nakayama, K., Surf. Sci., 36(1973) , 817.
14 West, L. A., J. Vac. Sci. Technol., 13(1976) , 198.
15 Oechsner, H., Z. Phys., 238(1970) , 433.
16 Penn, D. R., J. Electron Spectrosc. Relat. Phenom., 9(1976) , 29.
17 Oechsner, H., Z. Phys., 261 (1973) , 37.
18 Wood, B. J.; Wise, H., Surf. Sci., 52(1975) , 151.
19 Nagel, S. R.; Fisher, G. B.; Tauc, J.; Bagley, B. G., Phys. Rev., B13 (1976) , 3284.
20 Kelly, R., Surf. Sci., 100 (1980) , 85.b
No related articles found!