STUDY OF PREDOMINANCE PHASE DIAGRAM IN METALLURGY BY USING COMPUTER
by WANG Leshan; XU Zhihong (Institute of Chemical Metallurgy; Academia Sinica; Beijing); LI Danian (Institute of Science and Technology Information; Beljing) (Manuscript received 8 November; 1982; revised manuscript 3 May; 1983)
Cite this article: 

by WANG Leshan; XU Zhihong (Institute of Chemical Metallurgy; Academia Sinica; Beijing); LI Danian (Institute of Science and Technology Information; Beljing) (Manuscript received 8 November; 1982; revised manuscript 3 May; 1983). STUDY OF PREDOMINANCE PHASE DIAGRAM IN METALLURGY BY USING COMPUTER. Acta Metall Sin, 1984, 20(2): 188-198.

Download:  PDF(666KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In accordance with the idea of generalized phase rule, we have studied the necessary condition of existence of predominance area of phase diagram, in which the number of required message input has been reduced to minimum, and set up the computer program for automatically drawing and calculation. In this program system, it contains the following 7 functions: (1) automatically balance the stoichiometric constants of all possible reactions, (2) carry out the Gibb,s free energy calculation of all possible reactions, (3) automatically cancel out the non-existence phase in the designated condition, (4) calculate out all of the locations of 3 phase intersections, 2phase cross lines, (5) find out the phase name, (6) find out the temperature profiles to be interested in, and (7) select the appropriate parameters. This program system has been used in the field of pyrometaUugy for explaining how to select the best operating condition.
Received:  18 February 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I2/188

1 Linkson, P. B., Miner. Sci. Eng., 11 (1979) , 65.
2 张索林;梁植林,有色金属,34(1982) ,№2,65.
3 Linkson, P. B., Corros. Sci., 19(1979) , 613.
4 王乐珊;许志宏,化工冶金,(1980) ,№1,88.
5 Smith, J. M.; Van Ness, H. C., Introduction to Chemical Engineering Thermodynamics, McGraw-Hill, 1975, p. 415.
6 李大年;王乐珊;许志宏,计算机应用化学,1984,待发表.
7 张显鹏,第一届全国冶炼理论学术会议文集,1982,p.40.
8 魏寿昆,冶金过程热力学,上海科学技术出版社,1980,p.354.Z
No related articles found!
No Suggested Reading articles found!