ON THERMODYNAMIC CALCULATION OF Ms AND ON DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-C |
XU Zuyao(T. Y. Hsu); ZHANG Hongbing; LUO Shoufu (Shanghai Jiaotong University) (Manuscript received 7 February; 1983) |
|
Cite this article:
XU Zuyao(T. Y. Hsu); ZHANG Hongbing; LUO Shoufu (Shanghai Jiaotong University) (Manuscript received 7 February; 1983). ON THERMODYNAMIC CALCULATION OF Ms AND ON DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-C. Acta Metall Sin, 1984, 20(3): 151-161.
|
Abstract In order to suit the calculation with computer, △G_(Fe)~(γ-α) from various authors are formulated. Ms from various △G_(Fe)~(γ-α) and different models for evaluation of △G_(Fe)~(γ-α), e. g. refined Fither, KRC, LFG and Hsu's are obtained. Comparison is made among these results. The calculated Ms depends on not only the evaluation model of △G~(γ-α) but also △G_(Fe)~(γ-α). Both LFG treatment with △G_(Fe)~(γ-α) from Mogutnov and Hsu's model with △G_(Fe)~(γ-α) from Kaufman et al. are in good agreement with the experimental M_s. However Hsu's model is much simpler than the general accepted LFG's M_s of Fe-C with x_c=0.01 to 0.05 are detected rather accurately and they are consistent with that given by Kaufman et al. Ms of Fe-C with x_c=0.06 by Greninger seems too high. The calculated driving force depends on not only the evaluation model of △G~(γ-α) but also mainly △G_(Fe)~(γ-α) and M_s adopted. It is more likely that the driving force increases with the increament of carbon content.
|
Received: 18 March 1984
|
1 Xu Zuyao (T. Y. Hsu, 徐祖耀), Shanghai Jiao Tong University Treatise, Ⅰ, 1981, MS-003. 2 Fisher, J.C., Trans. AIME 185 (1949) , 688. 3 Kaufman, L.; Radcliffe, S. V.; Cohen, M., Decomposition of Austensite by Difusional Processes, Eds. Zackay, V.F.; Aaronson, H.I., Interscience Publ. 1962, p.313. 4 Fowler, R.H.; Guggenheim, E.A., Statistical Thermodynamics, New York, Cambridge University Press, 1939. 5 徐祖耀,金属学报,15(1979) ,329. 6 Kaufman, L.; Clougherty, E. V.; Weiss, R.J., Acta Metall., 11 (1963) , 323. 7 Orr, R. L.; Chipman, J., Trans. Metall. Soc. AIME, 239 (1967) , 630. 8 Mogutnov, B.M.; Tomilin, I. A.; Shvarsman, L.A., Thermodynamics of Fe-C Alloys, Metallurgy Press, Moscow, 1972, p.110. 9 Agren, J., Metall. Trans., 10A (1979) , 1847. 10 Greninger, A.B., Trans. ASM, 30 (1942) , 1. 11 Bhadeshia, H.K.D.H., Meta Sci., 15 (1981) , 175. 12 Lobo, J. A.; Geiger, G. H., Metall. Trans., 7A (1976) , 1347. 13 Lobo, J.A.; Geiger, G.H., Metall. Trans., 7A (1976) , 1359. 14 Bell, T.; Owen, W.S., Trans. Metall. Soc. AIME, 239 (1967) , 1940. 15 Zener, C., Trans. AIME, 167 (1946) , 513. 16 Shiflet, G.J.; Bradley, J.R.; Aaronson, H.I., Metall. Trans., 9A (1978) , 999. 17 Lacher, J.R., Proc. Cambridge Phils. Soc., 33 (1937) , 518. 18 McLellan, R.B.; Garrard, T. L.; Horowitz, S. J.; Sprague, J.A., Trans. Metall. Soc. AIME, 239(1967) , 528. 19 Aaronson, H.I.; Domain, H.A.; Pound, G.M., Trans. Metall. Soc. AIME, 236 (1966) , 753. 20 Bhadeshia, H.K.D.H., Met. Sci., 14 (1980) , 230.f |
No Suggested Reading articles found! |
|
|