Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (3): 151-161    DOI:
Current Issue | Archive | Adv Search |
ON THERMODYNAMIC CALCULATION OF Ms AND ON DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-C
XU Zuyao(T. Y. Hsu); ZHANG Hongbing; LUO Shoufu (Shanghai Jiaotong University) (Manuscript received 7 February; 1983)
Cite this article: 

XU Zuyao(T. Y. Hsu); ZHANG Hongbing; LUO Shoufu (Shanghai Jiaotong University) (Manuscript received 7 February; 1983). ON THERMODYNAMIC CALCULATION OF Ms AND ON DRIVING FORCE FOR MARTENSITIC TRANSFORMATION IN Fe-C. Acta Metall Sin, 1984, 20(3): 151-161.

Download:  PDF(870KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to suit the calculation with computer, △G_(Fe)~(γ-α) from various authors are formulated. Ms from various △G_(Fe)~(γ-α) and different models for evaluation of △G_(Fe)~(γ-α), e. g. refined Fither, KRC, LFG and Hsu's are obtained. Comparison is made among these results. The calculated Ms depends on not only the evaluation model of △G~(γ-α) but also △G_(Fe)~(γ-α). Both LFG treatment with △G_(Fe)~(γ-α) from Mogutnov and Hsu's model with △G_(Fe)~(γ-α) from Kaufman et al. are in good agreement with the experimental M_s. However Hsu's model is much simpler than the general accepted LFG's M_s of Fe-C with x_c=0.01 to 0.05 are detected rather accurately and they are consistent with that given by Kaufman et al. Ms of Fe-C with x_c=0.06 by Greninger seems too high. The calculated driving force depends on not only the evaluation model of △G~(γ-α) but also mainly △G_(Fe)~(γ-α) and M_s adopted. It is more likely that the driving force increases with the increament of carbon content.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/151

1 Xu Zuyao (T. Y. Hsu, 徐祖耀), Shanghai Jiao Tong University Treatise, Ⅰ, 1981, MS-003.
2 Fisher, J.C., Trans. AIME 185 (1949) , 688.
3 Kaufman, L.; Radcliffe, S. V.; Cohen, M., Decomposition of Austensite by Difusional Processes, Eds. Zackay, V.F.; Aaronson, H.I., Interscience Publ. 1962, p.313.
4 Fowler, R.H.; Guggenheim, E.A., Statistical Thermodynamics, New York, Cambridge University Press, 1939.
5 徐祖耀,金属学报,15(1979) ,329.
6 Kaufman, L.; Clougherty, E. V.; Weiss, R.J., Acta Metall., 11 (1963) , 323.
7 Orr, R. L.; Chipman, J., Trans. Metall. Soc. AIME, 239 (1967) , 630.
8 Mogutnov, B.M.; Tomilin, I. A.; Shvarsman, L.A., Thermodynamics of Fe-C Alloys, Metallurgy Press, Moscow, 1972, p.110.
9 Agren, J., Metall. Trans., 10A (1979) , 1847.
10 Greninger, A.B., Trans. ASM, 30 (1942) , 1.
11 Bhadeshia, H.K.D.H., Meta Sci., 15 (1981) , 175.
12 Lobo, J. A.; Geiger, G. H., Metall. Trans., 7A (1976) , 1347.
13 Lobo, J.A.; Geiger, G.H., Metall. Trans., 7A (1976) , 1359.
14 Bell, T.; Owen, W.S., Trans. Metall. Soc. AIME, 239 (1967) , 1940.
15 Zener, C., Trans. AIME, 167 (1946) , 513.
16 Shiflet, G.J.; Bradley, J.R.; Aaronson, H.I., Metall. Trans., 9A (1978) , 999.
17 Lacher, J.R., Proc. Cambridge Phils. Soc., 33 (1937) , 518.
18 McLellan, R.B.; Garrard, T. L.; Horowitz, S. J.; Sprague, J.A., Trans. Metall. Soc. AIME, 239(1967) , 528.
19 Aaronson, H.I.; Domain, H.A.; Pound, G.M., Trans. Metall. Soc. AIME, 236 (1966) , 753.
20 Bhadeshia, H.K.D.H., Met. Sci., 14 (1980) , 230.f
No related articles found!