Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (3): 169-284    DOI:
Current Issue | Archive | Adv Search |
CYCLIC DEFORMATION OF ALUMINUM POLYCRYSTALS
CHEN Xianfeng; LIN Donglian (T. L. Lin)(Shanghai Jaiotong University) (Manuscript received 11 March; 1983; revised manuscript 14 October; 1983)
Cite this article: 

CHEN Xianfeng; LIN Donglian (T. L. Lin)(Shanghai Jaiotong University) (Manuscript received 11 March; 1983; revised manuscript 14 October; 1983). CYCLIC DEFORMATION OF ALUMINUM POLYCRYSTALS. Acta Metall Sin, 1984, 20(3): 169-284.

Download:  PDF(3381KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The cyclic deformation behaviour of Al polycrystals has been investigated at constant plastic strain amplitudes, γ_(pl), over a range 2×10~(-5)<ε_(pl)<4.7×10~(-3). The cyclic hardening curves and the cyclic stress-strain curves were measured and correlated with the change of dislocation substructure in grains and grain boundaries. In this study, an effort.was taken to explore: @1. the change of dislocation substructure as a function of the number of cycles; @2. the effect of the strain amplitude on the dislocation substructure in saturation; and @3. the role of grain boundary in the cyclic deformation.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/169

1 Mughrabi, H.; Herz, K.; Ackerman, F., Proc. of 4th Int. Conf. on Strength of Metals and Alloys, Nancy, France, 1976, Vol.3, p.1244.
2 Mugharbi, H., Muter. Sci. Eng., 33 (1978) , 207.
3 Winter, A.T., Philos. Mag., 30 (1974) , 719.
4 Hancock, J. R.; Grosskreutz, J.C., Acta Metall., 17 (1969) , 77.
5 Kuhlmann-Wilsdorf, D., Mater. Sci. Eng., 27 (1977) , 137.
6 Mughrabi, H.; Wang, R. (王仁卉), Deformation of Polycrystals Mechanisms and Microstructures, Proc. of the 2nd Ris Int. Symp. on Metallurgy and Materials Science, Eds. Hansen, Horsewell, A.; Leffers, T.; et al., RIS National Laboratory, Roskilde, Denmark, 1981, p.87.
7 Rasmussen, K.V.; Pedersen, O.B. Proc. of 5th Int. Conf. on the Strength of Metals and Alloys, Eds. Haasen, P.; Gerald, V.; Kostorz, G., Aachen, 1979, Vol.2, p.1219.
8 Rasmussen, K.V.; Pedersen, O.B., Acta Metall., 28 (1980) , 1467.
9 Lukas, P.; Klesnil, M.,Mater. Sci. Eng., 11 (1973) , 345.
10 Figueroa, J.C.; Bhat, S.P.; de la Veaux, R.; Murzenski, S.; Lar Laird, C., Acta Metall., 29 (1981) , 1667.
11 Grosskreutz, J.C.; Mughrabi, H., Description of the Work-Hardened Structure at Low Temperature in Cyclic Deformation, in: Constitutive Equations in Plasticity, Ed. Argon, A. S., MITPress, Cambridge, Hassachusetts, 1975, p.251-326.
12 Winter, A.T.; Pedersen, O.B.; Rasmussen, K.V., Acta Metall., 29 (1981) , 735.
13 Snowden, K. U., Acta Metall., 11 (1963) , 675.
14 Grosskreutz, J.C.; Waldow, P., Acta Metall., 11 (1963) , 717.
15 Feltner, C.E., Acta Metall., 11 (1963) , 817.
16 Grosskreutz, J.C., J. Appl. Phys., 34 (1963) , 372.
No related articles found!