SUPERELASTICITY OF Ni-Ti ALLOY AND IN SITU OBSERVATION OF ITS PHASE TRANSITION BY SEM
JIN Jialing (Shanghai Institute of Iron and Steel Research) (Manuscript received 3 January; 1983; revised manuscript 30 July; 1983)
Cite this article: 

JIN Jialing (Shanghai Institute of Iron and Steel Research) (Manuscript received 3 January; 1983; revised manuscript 30 July; 1983). SUPERELASTICITY OF Ni-Ti ALLOY AND IN SITU OBSERVATION OF ITS PHASE TRANSITION BY SEM. Acta Metall Sin, 1984, 20(3): 176-181.

Download:  PDF(1500KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An in situ observation by SEM was made of the phase transition induced by stain in the specially heat treated 51.6 at.-%Ni-Ti ahoy of which the superelasticity might be reached to such extent of its maximum elastic strain up to 17%. The phase transition is shown as two stages, namely, pre-martensitic and martensitic. The alloy reveals a behaviour for superelasticity, i. e., if the strain exceeds no more than its elastic limit, the whole transition process may be reversible, and the macro-or micro-feature may be back to beginning after unloading at any point of the curve. However, the intergranular cracks and the internal slips may be appeared, as well as the unreversible residual strain may be then remained if it exceeded the limit.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/176

1 徐永波;李恒武;苏会和;朱桂秋,金属学报,15(1979) ,369.
2 Wayman, C.M., Proc. of 1st JIM Int. Symp. on New Aspects of Martensitic Transformation, Ed. Suzuki, H. et al., Sendal, JIM, 1976, p.159.
3 Ling, H.C.; Kaplow, R., Metall. Trans., 11A (1980) , 77.
4 Nakanishi, N., Prog. Mater. Sci., 24 (1979) , №3/4, 143.
5 Warlimont, H.; Delaey, L.; Krishnan, R.V.; Tas, H., J. Mater. Sci.; 9 (1974) , 1545.
6 Krishnan, R.V.; Delaey, L.; Tas, H.; Warlimont, H., J. Mater. Sci., 9 (1974) , 1536.S
No related articles found!
No Suggested Reading articles found!