| ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-Al_2O_3-CaF_2 SLAGS |
| WANG Changzhen; YE Shuqing; YU Dingyu; GUO Wenquan(Northeast University of Technology; Shenyang)(Manuscript 1 August; 1983; revised manuscript 20 December; 1983) |
|
Cite this article:
WANG Changzhen; YE Shuqing; YU Dingyu; GUO Wenquan(Northeast University of Technology; Shenyang)(Manuscript 1 August; 1983; revised manuscript 20 December; 1983). ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-Al_2O_3-CaF_2 SLAGS. Acta Metall Sin, 1984, 20(5): 357-364.
|
|
|
Abstract The activity of La_2O_3 in liquid slags of various composition of La_2O_3-Al_2O_3-CaF_2 ternary system has been determined by equilibrating the slag with liquid Sn in a graphite crucible under one atmosphere of CO at 1600℃ in Mo-wire furnace. The iso-activity diagram and the liquid boundary for La_2O_3 at 1600℃ were ascertained. It was resulted that the activity of La_2O_3 increases with the increase of CaF_2 concentration or with the decrease of Al_2O_3 concentration when the La_2O_3 concentration remained constant; and with the increase of La_2O_3 concentration when the concentration of OaF_2 and Al_2O_3 remained constant.
|
|
Received: 18 May 1984
|
1 王常珍;邹元爔,金属学报,16(1980) ,190. 2 王常珍;杨代银,金属学报,15(19179) ,433. 3 王渭源;邹元爔,金属学报,6(1963) ,40. 4 邹元爔;赵彭年;曹兆民,金属学报,6(1963) ,121. 5 Ernest, M.; Chou Yuanhsi(邹元爔); Chao Pengnian (赵彭年), Sci. Sinica, 11(1962) , 1287. 6 Chou Yuanhsi(邹元爔); Chow Jichcng(周继程); Chao Pengnian(赵彭年)Sci. Sinica, 12(1963) , 1249. 7 Levin, E. M.; Robbins, C. R.; McMurdie, H. F., Compiled at the National Burcanu of Standards, Eds. Reser, M. K., Am. Ceram. Soc., 2nd ed. 1969, p. 124, Fig. 312. 8 郭祝崑;严东生.硅酸盐学报,1(1962) ,1. 9 Levin, E. M.; Robbins, C. R.; McMurdie, H. F., Compiled at the National Bureau of Standards, Ed. Reser, M. K., Am. Ceram. Soc. 2nd ed. 1969, p. 470, Fig. 1673.] |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|