Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (5): 357-364    DOI:
Current Issue | Archive | Adv Search |
ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-Al_2O_3-CaF_2 SLAGS
WANG Changzhen; YE Shuqing; YU Dingyu; GUO Wenquan(Northeast University of Technology; Shenyang)(Manuscript 1 August; 1983; revised manuscript 20 December; 1983)
Cite this article: 

WANG Changzhen; YE Shuqing; YU Dingyu; GUO Wenquan(Northeast University of Technology; Shenyang)(Manuscript 1 August; 1983; revised manuscript 20 December; 1983). ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-Al_2O_3-CaF_2 SLAGS. Acta Metall Sin, 1984, 20(5): 357-364.

Download:  PDF(522KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The activity of La_2O_3 in liquid slags of various composition of La_2O_3-Al_2O_3-CaF_2 ternary system has been determined by equilibrating the slag with liquid Sn in a graphite crucible under one atmosphere of CO at 1600℃ in Mo-wire furnace. The iso-activity diagram and the liquid boundary for La_2O_3 at 1600℃ were ascertained. It was resulted that the activity of La_2O_3 increases with the increase of CaF_2 concentration or with the decrease of Al_2O_3 concentration when the La_2O_3 concentration remained constant; and with the increase of La_2O_3 concentration when the concentration of OaF_2 and Al_2O_3 remained constant.
Received:  18 May 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I5/357

1 王常珍;邹元爔,金属学报,16(1980) ,190.
2 王常珍;杨代银,金属学报,15(19179) ,433.
3 王渭源;邹元爔,金属学报,6(1963) ,40.
4 邹元爔;赵彭年;曹兆民,金属学报,6(1963) ,121.
5 Ernest, M.; Chou Yuanhsi(邹元爔); Chao Pengnian (赵彭年), Sci. Sinica, 11(1962) , 1287.
6 Chou Yuanhsi(邹元爔); Chow Jichcng(周继程); Chao Pengnian(赵彭年)Sci. Sinica, 12(1963) , 1249.
7 Levin, E. M.; Robbins, C. R.; McMurdie, H. F., Compiled at the National Burcanu of Standards, Eds. Reser, M. K., Am. Ceram. Soc., 2nd ed. 1969, p. 124, Fig. 312.
8 郭祝崑;严东生.硅酸盐学报,1(1962) ,1.
9 Levin, E. M.; Robbins, C. R.; McMurdie, H. F., Compiled at the National Bureau of Standards, Ed. Reser, M. K., Am. Ceram. Soc. 2nd ed. 1969, p. 470, Fig. 1673.]
No related articles found!
No Suggested Reading articles found!