| EFFECT OF Nb ON γ'-PHASE PRECIPITATIONHARDENED Ni-Cr-Al-Ti BASE SUPERALLOY |
| CHEN Shizhen; GUAN Changbin; KANG Datao (North-East Heavy Machinery Institute; Qiqihar); GONG Yansheng; LIU Jinyu (Oiqihar Steel Works)(Manuscript received 14 January; 1983; revised manuscript 13 January; 1984) |
|
Cite this article:
CHEN Shizhen; GUAN Changbin; KANG Datao (North-East Heavy Machinery Institute; Qiqihar); GONG Yansheng; LIU Jinyu (Oiqihar Steel Works)(Manuscript received 14 January; 1983; revised manuscript 13 January; 1984). EFFECT OF Nb ON γ'-PHASE PRECIPITATIONHARDENED Ni-Cr-Al-Ti BASE SUPERALLOY. Acta Metall Sin, 1984, 20(6): 398-488.
|
|
|
Abstract The effect of Nb content on the y'-phase precipitation-hardened Ni-Cr-Al-Ti base superaUoy has been investigated. Results show that a moderate addition of Nb could improve both strength and ductility of the superaUoy at room and high temperatures. It was ascertained that such improvement on the strength and ductility is made principally after the strengthening Y'-phase and the grain refinement respectively.
|
|
Received: 18 June 1984
|
1 冶军,美国镍基高温合金,科学出版社,1978,p.49,52. 2 原田広史;山崎道夫,鈇鋼,65(1979) ,1059. 3 Guo Encai; Ma Fujun, Superalloys 1980, Proc. of the 4th Int. Symp. on Superalloys, Pennsylvania, Eds. Tien, J. K.; Wlodek, S. T., et al., ASM, Metals Park, Ohio, 1980, p. 431. 4 島贯康,日本金属学会誌,43(1979) ,203. 5 Melander, A.; Persson, P. A., Met. Sci., 12(1978) , 391. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|