Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (3): 1-6    DOI:
Current Issue | Archive | Adv Search |
THE EFFECT OF PRIOR AUSTENITIC GRAIN BOUNDARIES ON NUCLEATION OF(225)_γ MARTENSITE IN STEELS
ZHANG Xingquan;HE Xianming Shanghai Polytechnic University No.2
Cite this article: 

ZHANG Xingquan;HE Xianming Shanghai Polytechnic University No.2. THE EFFECT OF PRIOR AUSTENITIC GRAIN BOUNDARIES ON NUCLEATION OF(225)_γ MARTENSITE IN STEELS. Acta Metall Sin, 1985, 21(3): 1-6.

Download:  PDF(1297KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Results are Presented for the relationship between the number of(225)_γ mar-tensite plates per unit volume,N_v,and the mean diameter of prior austenitegrain,D,for steel T10A and GCr15 being N_v=N_0 (?),where N_0 is a con-stant.This relationship may be derived by the theory of dislocation of plastic de-formation in polycrystal at lower temperature under applied driving force of phasetransformation.Accordingly,the nucleation of(225)_γ martensite is the result ofon set of the motion of dislocation source under the applied driving force of phasetransformation.Consequently,these might be no pre-existing martensite nucleus,but are pre-existing dislocation sources.The austenite grain refinement may bean effective method for refining the martensite plates.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/1

1 徐祖耀,马氏体相变与马氏体,科学出版社,1980年p.430-465.
2 Cohen,M.;Waymen,C.M.,Metallurgical Treatieses,Presentations at the USA-China Bilateral Conference,Sponsored by the Metallurgical Society of AIME,ASM and CSM to be Held in Beijing,November 13-22,1981,p.445.
3 Fullman,R.L.,Trans.AIME,197(1953) ,447.
4 Dehoff,R.T.;Rhines,F.W.,Trans Metall.Soc.AIME,22(1961) ,975.
5 洛阳轴承研究所,热处理手册,第二分册,机械工业出版社,1981年,p.278-295.
6 Frank,F.C.,Acta Metall.,1(1953) ,15.
7 Knapp,H.;Dehlinger,U.,Acta Metall.,4(1956) ,289.
8 张星泉;贺贤铭,淬火钢中微裂纹形成,待发表.
9 张星泉;苏宁,奥氏体成分不均匀细化马氏体模型,待发表.H
No related articles found!