Acta Metall Sin  1985, Vol. 21 Issue (3): 7-148    DOI:
Current Issue | Archive | Adv Search |
TEM STUDY OF SIX REPRESENTATIVE LOW CARBON MARTENSITI STEELS
TAN Yuxu Xi'an Jiaotong University
Cite this article: 

TAN Yuxu Xi'an Jiaotong University. TEM STUDY OF SIX REPRESENTATIVE LOW CARBON MARTENSITI STEELS. Acta Metall Sin, 1985, 21(3): 7-148.

Download:  PDF(3425KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Six representative low carbon martensitic steels were analyzed under TEM,Observations showed as follow:The thin retained austenite films usually exist in the structure of the low car-bon(namely,0.1—0.25 wt-%C)martensitic steels;ε-carbides formed in auto-tempering precipitate on the matrix of the lath mar-tensites;Internal twins exist in part of some lath matrix of the six steels;ε-carbides transform into cementites when tempered at 300-400℃.Cementitesform in three sites,lath boundaries,{110}_M planes and twin boundaries;Twins disappear when tempering temperature raise to 500℃ but the outlineof lath boundaries still keeps its original shape.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/7

1 松田昭一;井上泰;三村宏;冈村义弘,钢の强韧性,日本铁钢学会,日本金属学会编,Climax Molybdenum Development Co.(Jpn) Ltd.,1971,p.45.
2 Naylor,J.P.,Metall.Trans.,10A(1979) ,861.
3 Sandvik,B.P.J.;Wayman,C.M.,Metallography,16(1983) ,199.
4 Clark,R.A.;Thomas,G.,Metall.Trans.,6A(1975) ,696.
5 Bhadeshia,H.K.D.H.;Edmonds,D.V.,Met.Sci.,13(1979) ,325.
6 Speich,G.R.;Leslie,W.C.,Metall.Trans.,3(1972) ,1043.
7 Chilton,J.M.;Kelly,P.M.,Acta Metall.,16(1968) ,637.
8 Raghavan,M.;Thomas,G.,Metall.Trans.,10(1979) ,1665.
9 弘津祯彦,热处理,14(1974) ,323.
No related articles found!
No Suggested Reading articles found!