ON CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS ALLOY Fe_(100-x)P_x
WANG Jinhuan;WANG Ruyao;LI Xianyong Luoyang Institute of Technology
Cite this article: 

WANG Jinhuan;WANG Ruyao;LI Xianyong Luoyang Institute of Technology. ON CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS ALLOY Fe_(100-x)P_x. Acta Metall Sin, 1985, 21(3): 94-98.

Download:  PDF(1428KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The structure and crystallization on heating of the amorphous alloy Fe_(100-x)P_xduplicated film made by electrodeposition have been examined by DTA,TEM andX-ray diffraction.The observation on alloy Fe_(86)P_(14)which is approach to the eu-tectic composition of Fe-P system is shown as diffuse scattering ring pattern ofelectron diffraction and broadened peak of X-ray diffraction.The crystallization ofthe Fe_(100-x)P_(14)deposited film seems to be the processes of low temperature relaxa-tion,formation of supersaturated solution of α-Fe(P),precipitation of Fe_3P fromα-Fe(P)as well as formation of stable phases of α-Fe(P)and Fe_3P.The Fe_(86)P_(14)grain growth is initiated above 745℃ with a steady exothermal peak on DTAcurve.The initial temperature of crystallization of Fe_(100-x)P_x amorphous alloy in-creases and of precipitation of Fe_3P decreases with the increase of its P content.The initial crystallization temperature of Fe_(86)P_(14)is about 250℃.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/94

1 上平晓,日本专利,昭52-140403,(1977) .
2 王晋桓;王汝耀;刘泽勤,Fe-P电沉积非晶层的制备工艺,第三届非晶物理及材料学术讨论会论文,1982年.
3 Masumoto,T.;Kimura,H.;Inove,A.,Mater.Sci.Eng.,23(1976) ,141.
No related articles found!
No Suggested Reading articles found!