| ON CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS ALLOY Fe_(100-x)P_x |
| WANG Jinhuan;WANG Ruyao;LI Xianyong Luoyang Institute of Technology |
|
Cite this article:
WANG Jinhuan;WANG Ruyao;LI Xianyong Luoyang Institute of Technology. ON CRYSTALLIZATION OF ELECTRODEPOSITED AMORPHOUS ALLOY Fe_(100-x)P_x. Acta Metall Sin, 1985, 21(3): 94-98.
|
|
|
Abstract The structure and crystallization on heating of the amorphous alloy Fe_(100-x)P_xduplicated film made by electrodeposition have been examined by DTA,TEM andX-ray diffraction.The observation on alloy Fe_(86)P_(14)which is approach to the eu-tectic composition of Fe-P system is shown as diffuse scattering ring pattern ofelectron diffraction and broadened peak of X-ray diffraction.The crystallization ofthe Fe_(100-x)P_(14)deposited film seems to be the processes of low temperature relaxa-tion,formation of supersaturated solution of α-Fe(P),precipitation of Fe_3P fromα-Fe(P)as well as formation of stable phases of α-Fe(P)and Fe_3P.The Fe_(86)P_(14)grain growth is initiated above 745℃ with a steady exothermal peak on DTAcurve.The initial temperature of crystallization of Fe_(100-x)P_x amorphous alloy in-creases and of precipitation of Fe_3P decreases with the increase of its P content.The initial crystallization temperature of Fe_(86)P_(14)is about 250℃.
|
|
Received: 18 March 1985
|
1 上平晓,日本专利,昭52-140403,(1977) . 2 王晋桓;王汝耀;刘泽勤,Fe-P电沉积非晶层的制备工艺,第三届非晶物理及材料学术讨论会论文,1982年. 3 Masumoto,T.;Kimura,H.;Inove,A.,Mater.Sci.Eng.,23(1976) ,141. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|