Abstract A study in a certain range of temperature and strain rate was made of thePortevin-Le Chatelier effect in the sheet specimens as-quenched or further pur-posely aged for a short-term of a commercial Al alloyc ontaining 4.19% Cu and1.25% Mg.It resulted that the ripple marking formation on the surface of thesheet may be delayed by the further short-term aging after quenching.Thus,thedynamic strain aging process is likely to delay the happening of inhomogeneousdeformation band on the alloy sheet.
|
Received: 18 April 1985
|
1 Van Den Beukel,A.,Phys.Status Solidi,(a)30(1975) ,197. 2 塚田晴一;井上稔;高桥明男,塑性加工,15(1974) ,526. 3 Couchman,P.R.;Reynolds,C.L.,Jr.,Philos.Mag.,34(1976) ,327. 4 Miura B,Mechanical Behavior of Materials,Proc.of the Int.Conf.on Mechanical Behavior of Materials,Vol.1,JSMS,1972,p.128. 5 Mukherjee,K.;May,T.;D' Antonic,C.;Maciag,R.J.,Metall.Trans.1(1970) ,3233. 6 Kimura,H.;Kimura,A.;Hasiguti,R.R.,Acta Metall.,10(1962) 607. 7 King,J.E.;You,C.P.;Knott,J.F.,Acta Metall.,29(1981) ,1553. |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|