PORTEVIN-LE CHATELIER EFFECT IN COMMERCIAL AI-Cu-Mg ALLOY
ZHANG Caipei;WANG Hongxiang;WANG Jiyao;LAI Zuhan Northeast Institute of Technology;Shenyang
Cite this article: 

ZHANG Caipei;WANG Hongxiang;WANG Jiyao;LAI Zuhan Northeast Institute of Technology;Shenyang. PORTEVIN-LE CHATELIER EFFECT IN COMMERCIAL AI-Cu-Mg ALLOY. Acta Metall Sin, 1985, 21(4): 1-7.

Download:  PDF(683KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study in a certain range of temperature and strain rate was made of thePortevin-Le Chatelier effect in the sheet specimens as-quenched or further pur-posely aged for a short-term of a commercial Al alloyc ontaining 4.19% Cu and1.25% Mg.It resulted that the ripple marking formation on the surface of thesheet may be delayed by the further short-term aging after quenching.Thus,thedynamic strain aging process is likely to delay the happening of inhomogeneousdeformation band on the alloy sheet.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/1

1 Van Den Beukel,A.,Phys.Status Solidi,(a)30(1975) ,197.
2 塚田晴一;井上稔;高桥明男,塑性加工,15(1974) ,526.
3 Couchman,P.R.;Reynolds,C.L.,Jr.,Philos.Mag.,34(1976) ,327.
4 Miura B,Mechanical Behavior of Materials,Proc.of the Int.Conf.on Mechanical Behavior of Materials,Vol.1,JSMS,1972,p.128.
5 Mukherjee,K.;May,T.;D' Antonic,C.;Maciag,R.J.,Metall.Trans.1(1970) ,3233.
6 Kimura,H.;Kimura,A.;Hasiguti,R.R.,Acta Metall.,10(1962) 607.
7 King,J.E.;You,C.P.;Knott,J.F.,Acta Metall.,29(1981) ,1553.
No related articles found!
No Suggested Reading articles found!