Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (6): 100-104    DOI:
Current Issue | Archive | Adv Search |
MAGNETIC MOMENT OF AMORPHOUS CoP ALLOYS
by ZHAN Wenshan;SHEN Baogen;GUO Huiqun;ZHANG Zhiying Institute of Physics; Academia Sinico; Beijing
Cite this article: 

by ZHAN Wenshan;SHEN Baogen;GUO Huiqun;ZHANG Zhiying Institute of Physics; Academia Sinico; Beijing. MAGNETIC MOMENT OF AMORPHOUS CoP ALLOYS. Acta Metall Sin, 1985, 21(6): 100-104.

Download:  PDF(317KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The temperature dependence of the saturation magnetization of amorphousCo_(100-x)P_x (x=13.9-27.7) alloys prepared by electrodeposition was measured by amagnetic balance in the field 12 kOe between 77 and 1300K. The average magneticmoment per Co atom, from low temperature measurements, decreases withthe increase of P content. The effect of P cothent on 3d magnetic moment in Coatom was discussed on the basis of the electron transfer model and the change ofcoordination number of nearest-neighbour Co atom around the central Co atom.
Received:  18 June 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I6/100

1 Dietz, G., J. Magn. Magn. Mater., 6 (1977) , 47.
2 Bagley, B. G.; Turnbull, D., Bull. Am. Phys Soc., Ser. II, 10 (1965) , 1101.
3 Dietz, G.; Klett, K., J. Magn. Magn. Mater., 8(1978) , 57.
4 Dietz, G.; Bestgen, H., J. Magn. Magn. Mater., 19 (1980) , 157.
S De Lau, J. G. M., J. Appl. Phys., 41(1970) , 5355.
6 Cargill, G. S.; Cochrane, R. W., Amorphous Magnetism, Eds. Hooper, H. O.; De Craaf, A. M., Plenum, New York, 1973, p. 313.
7 Pan, D.; Turnbull, D., J. Appl. Phys., 45(1974) , 1406.
8 Cochrane, R. W.; Harris, R.; Stroem-Oison, J. O.: Zuckermann, M. J., Phys. Rev. Lett., 35(1975) , 676.
9 Mangin, Ph.; Marchal, G., J. Appl. Phys., 49 (1978) , 1709.C
No related articles found!