Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (6): 95-99    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF INITIAL CRYSTALLIZATION ON MAGNETIZATION OF METALLIC GLASSES(Fe_(1-x)Co_x)_(78)Si_(10)B_(12)
by CHEN Duxing;MA Mingtu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing;NING Taishan Institute of Physics; Academia Sinica; Beijing
Cite this article: 

by CHEN Duxing;MA Mingtu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing;NING Taishan Institute of Physics; Academia Sinica; Beijing. EFFECT OF INITIAL CRYSTALLIZATION ON MAGNETIZATION OF METALLIC GLASSES(Fe_(1-x)Co_x)_(78)Si_(10)B_(12). Acta Metall Sin, 1985, 21(6): 95-99.

Download:  PDF(1085KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The magnetizations, M_8 and M_(20), at the field H=8 and 20 kA/m respective-ly, of ribbon metallic glasses (Fe_(1-x) Co_x)_(78)Si_(10)B_(12) (x=0.1, 0.5, 0.7 and 1) afterannealed at T_a=350-500℃ have been measured. It was found that the initialcrystallization makes the saturation magnetizing of the metallic glasses hard, andthe M_(20) of them with x=0 and 1 decrease but with x=0.5 and 0.7 increase. Thisseems to be. explained by a magnetocrystalline anisotropy in the crystallite ofFe_(1-x)Co_x and a stress anisotropy in amorphous matrix.
Received:  18 June 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I6/95

1 井上明久;增本健;菊地纪雄;峰村哲郎,日本金属学会志,42(1978) ,294.
2 陈笃行,仪器仪表学报,5(1984) ,138.
3 ASTM Powder Diffraction File, 6-696; 5-727.
4 Morimoto, S.; Torikai, E.; Ito, A.; Shiiki, K.: Kudo, M., J. Magn. Magn. Mater., 31-34 (1983) , 1519.
5 Hatta, S.; Egami, T.; Graham, C. D., Jr., IEEE Trans. Magn., MAG-14 (1978) , 1013.
6 Bozorth, R. M., Ferromagnetism, D. Van Nostrand, New York, 1956, p. 194.
7 近角聪信;他编集,磁性体, 朝仓, 1975, p. 781.
8 Zijlstra, H., Experimental Methods in Magnetism, North-Holland, Amsterdam, 1967, Chap. 5.
No related articles found!
No Suggested Reading articles found!