Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (2): 68-74    DOI:
Current Issue | Archive | Adv Search |
EQUILIBRIUM OF Fe-La-O-S SYSTEM
CHEN Dong; HAN Qiyong; WANG Tao; XIANG Changxiang (Beijing University of Iron and Steel Technology)
Cite this article: 

CHEN Dong; HAN Qiyong; WANG Tao; XIANG Changxiang (Beijing University of Iron and Steel Technology). EQUILIBRIUM OF Fe-La-O-S SYSTEM. Acta Metall Sin, 1986, 22(2): 68-74.

Download:  PDF(535KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study was made of the equilibrium of Fe-La-O-S system. The oxygen activity was directly measured by the solid electrolyte sensors made of ZrO_2(MgO) tube. The stability of La_2O_2S in the electrolytic separation and the content of La as dissolved state in liquid iron were examined by means of radioassay and electrolytic isolation of inclusion in organic electrolyte under low temperature. By extrapolation of data obtained, the equilibrium constant of La_2O_2S may be described as: 1550℃ K_(La_2O_2S)=3.81×10~(-19) e_s~(La)=-4.1 1600℃ K_(La_2O_2S)=6.45×10~(-19) e_s~(La)=-4.8 1650℃ K_(La_2O_2S)=7.41×10~(-19) e_s~(La)=-4.2 La(1)=[La] △G_(sol)~0=-136700+59.82T, γ_(La)~0=0.33 (1873 K) It seems that the deoxysulphurizing effect of La is more intense than that of Co, Nd and Y.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/68

1 Vahed, A.; Kay, D.R., Metall. Trans. B, 7B (1976) , 375.
2 王常珍;王福珍;杜英敏;张小平,金属学报,16 (1980) ,83.
3 董元篪,北京钢铁学院研究生毕业论文,1981.
4 项长祥,北京钢铁学院研究生毕业论文,1981.
5 杨斯馥,北京钢铁学院研究生毕业论文,1982.
6 韩其勇等, Proc. of Sino-Jpn. Symp. on Steelmaking. Beijing, 1981. p, 25.
7 江岛等,铁钢,63 (1977) , 943.
8 Worrell, W.L.; Chipman, J., Trans. Metall. Soc. AIME, 230 (1964) , 1682.
9 #12
10 杜挺,中国金属学会冶金过程物理化学学术会议论文,1980.
11 Fischer, W.A., Arch. Eisenhuttenwes., 49 (1978) , 425.
12 韩其勇,球铁。1980,№2,31.
13 韩其勇;刘士伟;牛红兵;唐志伟,Proc. of First China-USA Bilateral Metallurgical Conf., Beijing, 1981, p. 192.
14 丰锡安,北京钢铁学院研究生毕业论文,1982.
15 Wilson, W.G., et al, J. Met., 26 (1974) , №5, 14.
16 Schindlerva, V.; Buzek, Z., Hutn. Listy, 25 (1970) , №5, 316.
17 Buzek, Z., Chemical Metallurgy of Iron Steel, ISJ, London, 1973, p. 174. ; Buzek, Z., Hutn. Listy, 29 (1974) , 784.
18 Ejima, A., et al., Trans. Iron Steel Inst. Jpn., 17 (1977) , 349.
19 Vahed, A.; et al., Metall. Trans., 7B (1976) , 375.
20 Elliott, J.F., et al., Thermochemistry for Steelmaking, Addison-Wesley, 1963, p. 410.
21 Sigworth, G.K.; Elliott, J.F., Met. Sci., 8 (1974) , 298.
No related articles found!
No Suggested Reading articles found!