EFFECT OF CARBON CONTENT ON AXI-CORED INTERGRANULAR CRACKS OF STEEL INGOT
QI Shangming; ZHENG Guoxue (Institute of Xining Steel Works); SHI Naili (Ma' anshan Institute of Iron and Steel Technology)
Cite this article: 

QI Shangming; ZHENG Guoxue (Institute of Xining Steel Works); SHI Naili (Ma' anshan Institute of Iron and Steel Technology). EFFECT OF CARBON CONTENT ON AXI-CORED INTERGRANULAR CRACKS OF STEEL INGOT. Acta Metall Sin, 1986, 22(2): 75-154.

Download:  PDF(3850KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An account was discussed of the nature of intergranular cracks appeared in the axial core of ingot of low carbon alloy steels, such as Cr5Mo, 12CrMoV and steel 10 on the basis of informations of industrial production and laboratory test. The experimental steel ingots weighing about 25 kg were examined under macroscopic observation, fractography, metallography and EMPA. It showed that the intergranular crack in axial core is true crack which seems to be related to the carbon content in steel owing to the high temperature δ→γ transformation on the solidification of ingot.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/75

1 田继丰;刘兴志;魏堃,金属学报,14 (1978) ,171
2 金属研究所;大连钢厂联合研究组,金属学报,14 (1978) ,165.
3 冶金部钢铁研究院;北京钢厂;齐齐哈尔钢厂合编,合金钢断口金相图谱,科学出版社,1979,p.54.
4 #12
No related articles found!
No Suggested Reading articles found!